Nanoindentation Under Dynamic Conditions

This material is based upon work supported under a National Science Foundation Graduate Research Fellowship. Any opinions, findings, conclusions or recommendations expressed in this publication are those of the author(s) and do not necessarily reflect the views of the National Science Foundation. Additional support for this work was provided by funding from the Atomic Weapons Establishment.

[1]  G. Sundararajan,et al.  A comparative study of tribological behavior of microarc oxidation and hard-anodized coatings , 2006 .

[2]  Etienne Patoor,et al.  Strain rate sensitivity in superelasticity , 2000 .

[3]  P. Dearnley,et al.  The sliding wear resistance and frictional characteristics of surface modified aluminium alloys under extreme pressure , 1999 .

[4]  Z. Luo,et al.  Structure and antiwear behavior of micro-arc oxidized coatings on aluminum alloy , 2002 .

[5]  T. Page,et al.  Measuring and modelling the instrumented indentation (nanoindentation) response of coated systems , 2006 .

[6]  R. Kirchheim INTERACTION OF HYDROGEN WITH DISLOCATIONS IN PALLADIUM—I. ACTIVITY AND DIFFUSIVITY AND THEIR PHENOMENOLOGICAL INTERPRETATION , 1981 .

[7]  P. F. Chester,et al.  Some Observations: , 2020, Soldiers of Destruction.

[8]  E. Seymour,et al.  NMR Measurement of Hydrogen Diffusion inβ-Palladium Hydride , 1975 .

[9]  C. D. The Hardness of Metals and its Measurement , 1935, Nature.

[10]  G. Subhash,et al.  Dynamic Vickers indentation of brittle materials , 2000 .

[11]  G. Sundararajan,et al.  A dynamic indentation technique for the characterization of the high strain rate plastic flow behaviour of ductile metals and alloys , 1991 .

[12]  F. A. Lewis,et al.  Hydrogen in palladium and palladium alloys , 1996 .

[13]  E. A. Owen,et al.  The palladium-hydrogen system , 1937 .

[14]  T. Page,et al.  Scratch deformation response of thin CNx coatings at ultra-low loads , 1998 .

[15]  G. Sundararajan,et al.  The localization of plastic flow under dynamic indentation conditions: I. Experimental results , 2006 .

[16]  J. Shaw,et al.  Thermomechanical aspects of NiTi , 1995 .

[17]  I. Schmidt A phenomenological model for superelastic NiTi wires based on plasticity with focus on strain-rate dependency caused by temperature , 2006 .

[18]  D. Tabor A simple theory of static and dynamic hardness , 1948, Proceedings of the Royal Society of London. Series A. Mathematical and Physical Sciences.

[19]  T. Clyne,et al.  Indentation characteristics of superelastic nickel-titanium wires and a preliminary study of copper-bonded joints between them , 2004, SPIE Smart Structures and Materials + Nondestructive Evaluation and Health Monitoring.

[20]  G. Thompson,et al.  Destruction of coating material during spark anodizing of titanium , 2006 .

[21]  J. Nobre,et al.  A study on elasto-plastic impact friction , 1999 .

[22]  H. Habazaki,et al.  Spark anodizing of β-Ti alloy for wear-resistant coating , 2007 .

[23]  Subra Suresh,et al.  Analysis of the impact of a sharp indenter , 2002 .

[24]  M. Laugier The development of the scratch test technique for the determination of the adhesion of coatings , 1981 .

[25]  A. Matthews,et al.  Characterisation of oxide films produced by plasma electrolytic oxidation of a Ti–6Al–4V alloy , 2000 .

[26]  M. V. Gol’tsova Reverse hydride transformations in the Pd–H system , 2006 .

[27]  T. W. Clyne,et al.  Thermo-physical properties of plasma electrolytic oxide coatings on aluminium , 2005 .

[28]  Steven J. Savage,et al.  ENGINEERING ASPECTS OF SHAPE MEMORY ALLOYS , 1991 .

[29]  J. Smith,et al.  Micro-Impact Testing: A New Technique for Investigating Thin Film Toughness, Adhesion, Erosive Wear Resistance, and Dynamic Hardness , 2001 .

[30]  Steve Bull,et al.  Can scratch testing be used as a model for the abrasive wear of hard coatings , 1999 .

[31]  T. W. Clyne,et al.  The thermal conductivity of plasma electrolytic oxide coatings on aluminium and magnesium , 2005 .

[32]  A. Matthews,et al.  Plasma electrolysis for surface engineering , 1999 .

[33]  Eric Finot,et al.  Monitoring the chemical changes in Pd induced by hydrogen absorption using microcantilevers. , 2003, Ultramicroscopy.

[34]  H. Wipf,et al.  Diffusion of hydrogen in metals , 1981 .

[35]  T. Clyne,et al.  Mullite-rich plasma electrolytic oxide coatings for thermal barrier applications , 2007 .

[36]  S. Nemat-Nasser,et al.  Superelastic and cyclic response of NiTi SMA at various strain rates and temperatures , 2006 .

[37]  A. Matthews,et al.  Kinetic aspects of aluminium titanate layer formation on titanium alloys by plasma electrolytic oxidation , 2002 .

[38]  Mark Gee,et al.  Low load multiple scratch tests of ceramics and hard metals , 2001 .

[39]  A. Matthews,et al.  Abrasive wear/corrosion properties and TEM analysis of Al2O3 coatings fabricated using plasma electrolysis , 2002 .

[40]  V. Goltsov The phenomenon of controllable hydrogen phase naklep and the prospects for its use in metal science and engineering , 1981 .

[41]  Fu-ping Wang,et al.  Oxidation behavior of ceramic coatings on Ti–6Al–4V by micro-plasma oxidation , 2007 .

[42]  G. Thompson,et al.  Tracing locations of new coating material during spark anodizing of titanium , 2006 .

[43]  H. Peisl,et al.  Lattice strains due to hydrogen in metals , 1978 .

[44]  H. C. Jamieson,et al.  The β → α phase transformation in palladium-hydrogen alloys , 1976 .

[45]  Nancy A. Winfree,et al.  Compressive superelastic behavior of a NiTi shape memory alloy at strain rates of 0.001–750 s−1 , 2001 .

[46]  Sia Nemat-Nasser,et al.  High Strain-Rate, Small Strain Response of a NiTi Shape-Memory Alloy , 2005 .

[47]  Sia Nemat-Nasser,et al.  Very high strain-rate response of a NiTi shape-memory alloy , 2005 .

[48]  A. Yerokhin,et al.  Phase formation in ceramic coatings during plasma electrolytic oxidation of aluminium alloys , 1998 .

[49]  Y. Sul,et al.  The significance of the surface properties of oxidized titanium to the bone response: special emphasis on potential biochemical bonding of oxidized titanium implant. , 2003, Biomaterials.

[50]  D. S. Rickerby,et al.  The relationship between hardness and scratch adhession , 1987 .

[51]  Jeff Perkins,et al.  Shape memory effects in alloys : [proceedings of the International Symposium on Shape Memory Effects and Applications held in Toronto, Ontario, Canada, May 19-22, 1975] , 1975 .

[52]  Ferdinando Auricchio,et al.  Shape-memory alloys: macromodelling and numerical simulations of the superelastic behavior , 1997 .

[53]  J. Smith,et al.  Investigating the fracture resistance and adhesion of DLC films with micro-impact testing , 2002 .

[54]  Y. .. Wang,et al.  Microarc oxidation coatings formed on Ti6Al4V in Na2SiO3 system solution: Microstructure, mechanical and tribological properties , 2006 .

[55]  Hisaaki Tobushi,et al.  Influence of strain rate on superelastic properties of TiNi shape memory alloy , 1998 .

[56]  M. K. Wilkinson,et al.  Neutron-diffraction observations on the palladium-hydrogen and palladium-deuterium systems , 1957 .

[57]  J.-H. You,et al.  Nanoindention response of superelastic materials , 2004, SPIE Micro + Nano Materials, Devices, and Applications.

[58]  K. E. Mironov Interstitial alloys , 1969 .

[59]  W. Xue,et al.  Microstructure and Phase Composition of Microarc Oxidation Coatings Formed on Ti–6Al–4V Alloy in Aluminate Solution , 2001 .

[60]  N. Bourne,et al.  Behavior of the shape memory alloy NiTi during one-dimensional shock loading , 2002 .

[61]  B. Beake,et al.  Nano-impact testing: an effective tool for assessing the resistance of advanced wear-resistant coatings to fatigue failure and delamination , 2004 .

[62]  K. Rebeiz,et al.  Influence of partial hydride formation/decomposition on the mechanical properties of palladium , 1996 .

[63]  Subra Suresh,et al.  DETERMINATION OF ELASTOPLASTIC PROPERTIES BY INSTRUMENTED SHARP INDENTATION , 1999 .

[64]  B. Beake Evaluation of the fracture resistance of DLC coatings on tool steel under dynamic loading , 2005 .

[65]  A. Matthews,et al.  Thickness effects on the mechanical properties of micro-arc discharge oxide coatings on aluminium alloys , 1999 .

[66]  T. Clyne,et al.  Nanoindentation of binary and ternary Ni–Ti-based shape memory alloy thin films , 2008 .

[67]  J. Nobre,et al.  Resistance of a ductile steel surface to spherical normal impact indentation: use of a pendulum machine , 1997 .

[68]  Ho-Jun Song,et al.  Fabrication of BaTiO3 films on titanium by microarc oxidation method and improvement of bioactivity by electric poling treatment , 2007 .

[69]  Y. Gong,et al.  Biomimetic coating of compound titania and hydroxyapatite on titanium. , 2007, Journal of biomedical materials research. Part A.

[70]  Chuanzhong Chen,et al.  RESEARCH STATUS ABOUT SURFACE MODIFICATION OF BIOMEDICAL Ti AND ITS ALLOYS BY MICRO-ARC OXIDATION , 2006 .

[71]  G. Sundararajan,et al.  The localization of plastic flow under dynamic indentation conditions-II. Analysis of results , 2006 .

[72]  P. H. Shipway Tribology: Friction and Wear of Engineering Materials , 1992 .

[73]  Fu-ping Wang,et al.  Study on corrosion resistance and roughness of micro-plasma oxidation ceramic coatings on Ti alloy by EIS technique , 2007 .

[74]  T. Clyne,et al.  Porosity in plasma electrolytic oxide coatings , 2006 .

[75]  Yaming Wang,et al.  Fretting wear behaviour of microarc oxidation coatings formed on titanium alloy against steel in unlubrication and oil lubrication , 2006 .

[76]  H. Tobushi,et al.  Temperature measurement as a new technique applied to the phase transformation study in a TiNi shape memory alloy subjected to tension , 2005 .

[77]  A. Yerokhin,et al.  Characterization of wear protective AlSiO coatings formed on Al-based alloys by micro-arc discharge treatment , 1996 .

[78]  Jun Lu,et al.  Dynamic indentation for determining the strain rate sensitivity of metals , 2003 .

[79]  B. Beake,et al.  Micro-impact testing: a new technique for investigating fracture toughness , 2001 .

[80]  Ferdinando Auricchio,et al.  Shape-memory alloys: modelling and numerical simulations of the finite-strain superelastic behavior , 1997 .

[81]  P. Vacher,et al.  Homogeneous and heterogeneous deformation mechanisms in an austenitic polycrystalline Ti-50.8 at% Ni thin tube under tension. Investigation via temperature and strain fields measurements , 2007 .

[82]  B. Koeppel,et al.  Dynamic Indentation Hardness and Rate Sensitivity in Metals , 1999 .

[83]  Yu Zhou,et al.  Characteristic and in vitro bioactivity of a microarc-oxidized TiO(2)-based coating after chemical treatment. , 2007, Acta biomaterialia.

[84]  J. Z. Zhang,et al.  Porous films on surface of titanium prepared by low voltage micro arc oxidation , 2007 .

[85]  Brian J. Koeppel,et al.  Characteristics of residual plastic zone under static and dynamic Vickers indentations , 1999 .

[86]  S. Gnedenkov,et al.  Composition and adhesion of protective coatings on aluminum , 2001 .

[87]  D. Fingerle,et al.  Ceramic materials for engines , 1987 .

[88]  L. Rama Krishna,et al.  The tribological performance of ultra-hard ceramic composite coatings obtained through microarc oxidation , 2003 .