Synthesis of dense WSi2 and WSi2-xvol.%SiC composites by high-frequency induction heated combustion and its mechanical properties
暂无分享,去创建一个
I. Shon | Jinsik Yoon | In-Yong Ko | H. Kim | D. Oh
[1] I. Shon,et al. Comparison of sintering behavior and mechanical properties between WC−8Co and WC−8Ni hard materials produced by high-frequency induction heating sintering , 2006 .
[2] J. Han,et al. Low-temperature cyclic oxidation behavior of MoSi2/SiC nanocomposite coating formed on Mo substrate , 2004 .
[3] I. Shon,et al. Synthesis of WC and dense WC–5 vol.% Co hard materials by high-frequency induction heated combustion , 2004 .
[4] I. Shon,et al. Synthesis of WC and dense WC–xvol.%Co hard materials by high-frequency induction heated combustion method , 2004 .
[5] W. Pan,et al. Fabrication and mechanical evaluation of SiC–TiC nanocomposites by SPS , 2004 .
[6] K. J. Rao,et al. Microwave sintering of MoSi2–SiC composites , 2003 .
[7] Z. A. Munir,et al. One-step synthesis of dense tungsten carbide-cobalt hard materials , 2002 .
[8] Z. A. Munir,et al. Synthesis of WSi2–ZrO2 and WSi2–Nb composites by field-activated combustion , 2001 .
[9] Z. A. Munir,et al. Dense WSi2 and WSi2–20 vol.% ZrO2 composite synthesized by pressure-assisted field-activated combustion , 2001 .
[10] I. Shon,et al. Simultaneous synthesis and densification of WSi2 and WSi2-20vol.%Nb composite by field-activated and pressure-assisted combustion , 2000 .
[11] G. S. Upadhyaya,et al. Synthesis and sintering of TiB2 and TiB2–TiC composite under high pressure , 2000 .
[12] Zuhair A. Munir,et al. Simultaneous synthesis and densification of Ti5Si3 and Ti5Si3–20 vol% ZrO2 composites by field-activated and pressure-assisted combustion , 1999 .
[13] 최상욱,et al. 고압 연소소결(HPCS)법을 이용한 Ti-C-Mo계 탄화물 복합체의 제조 , 1999 .
[14] Kazuo Yamazaki,et al. Simultaneous Synthesis and Densification of MoSi2 by Field‐Activated Combustion , 1996 .
[15] Y. Mahajan,et al. Reaction Hot Pressing and Characterization of MoSi2/SiCp Composites , 1995 .
[16] R. Abbaschian,et al. Toughening MoSi2 with niobium metal-effects of size and orientation of ductile laminae , 1994 .
[17] M. Hoffmann,et al. Mechanical properties of hot-pressed SiC-TiB2/TiC composites synthesizedin situ , 1993 .
[18] M. Hoffmann,et al. Sintering of in‐Situ Synthesized Sic–TiB2 Composites with Improved Fracture Toughness , 1992 .
[19] Mattheiss. Calculated structural properties of CrSi2, MoSi2, and WSi2. , 1992, Physical review. B, Condensed matter.
[20] J. Petrovic,et al. Hardness and Fracture Toughness of SiC‐Particle‐Reinforced MoSi2 Composites , 1991 .
[21] A. Berndt. Binary phase diagrams , 1969 .