Friction and wear properties of polymer, metal, and ceramic prosthetic joint materials evaluated on a multichannel screening device.

A 12-channel wear screening device was used to compare the wear properties of a variety of prosthetic joint materials. Two types of tests were run: (1) Ultrahigh molecular weight (UHMW) polyethylene bearing against metal or ceramic counterfaces and (2) various polymers bearing against 316 stainless steel as a standard counterface. Wear was quantified by weighing the polymer specimens, with presoaking and control-soak specimens used to minimize the error due to fluid absorption. The specimens were lubricated with bovine blood serum. Friction and polyethylene wear was very low with each of the metals (316 stainless steel, cobalt-chrome alloy, multiphase alloy, and titanium 6-4 alloy) such that the differences in wear rate would not be significant in terms of choosing a material for clinical application. However, titanium 6-4 alloy was found to be especially susceptible to abrasive wear by particles of acrylic cement. Nitrided titanium 6-4 counterfaces were impervious to acrylic abrasion. Polyethylene wear against highly polished, fully dense ceramics (Sialon, Alumina, Macor, and pyrolytic graphite) was as low as that with the metal counterfaces. Wear increased slightly with increasing ceramic surface roughness. The coefficient of friction of polyethylene against pyrolytic graphite was two to three times higher than with the metals or other ceramics. All of the alternate polymers underwent more wear than UHMW polyethylene. Teflon and polyester, two polymers that have proven unsuccessful in prior clinical use, had wear rates 1,600 and 830 times greater than polyethylene, respectively, an indication that the laboratory wear test provided a quantitative prediction of the behavior of the materials in vivo. However, it was difficult to assess the clinical significance of the less extreme wear rates since the ability of the tissues encapsulating a prosthesis to accomodate wear debris is not known on a quantitative basis.

[1]  H. Amstutz Polymers as bearing materials for total hip replacement: a friction and wear analysis. , 1969, Journal of biomedical materials research.

[2]  J. Dumbleton,et al.  A comparative evaluation of the wear of ultra-high molecular weight polyethylene abraded by Ti-6Al-4V , 1974 .

[3]  J. Dumbleton,et al.  The friction and wear behavior of irradiated very high molecular weight polyethylene , 1974 .

[4]  J. Charnley,et al.  Rate of wear in total hip replacement. , 1975, Clinical orthopaedics and related research.

[5]  J. Dumbleton,et al.  The friction and wear behavior of polyoxymethylene in connection with joint replacement , 1976 .

[6]  J. Galante,et al.  Some new studies of the wear behavior of ultrahigh molecular weight polyethylene. , 1976, Journal of biomedical materials research.

[7]  M Semlitsch,et al.  New prospects for a prolonged functional life-span of artificial hip joints by using the material combination polyethylene/aluminium oxide ceramin/metal. , 1977, Journal of biomedical materials research.

[8]  I C Clarke,et al.  Wear characteristics of UHMW polyethylene: a method for accurately measuring extremely low wear rates. , 1978, Journal of biomedical materials research.

[9]  M. Mayor,et al.  The biocompatibility of materials for internal fixation of fractures. , 1978, Journal of biomedical materials research.

[10]  J. Dumbleton Delrin as a Material for Joint Prostheses—A Review , 1979 .

[11]  J. Galante,et al.  Indentation creep of polymers for human joint applications. , 1979, Journal of biomedical materials research.

[12]  W. Jones,et al.  Effect of Sterilization Irradiation on Friction and Wear of Ultrahigh-Molecular-Weight Polyethylene. , 1979 .

[13]  R. Rose,et al.  The effects of radiation sterilization on the properties of ultrahigh molecular weight polyethylene. , 1979, Journal of biomedical materials research.

[14]  I. Clarke,et al.  Development of a ceramic surface replacement for the hip. An experimental Sialon model. , 1979, Biomaterials, medical devices, and artificial organs.

[15]  J. Galante,et al.  Contact pressure dependence of wear rates of ultra high molecular weight polyethylene. , 1979, Journal of biomedical materials research.

[16]  R. Cicek,et al.  Materials for internal prostheses: the present position and possible future developments. , 1980, Biomaterials.