Gelatin-derived bioadhesives for closing skin wounds: an in vivo study.

Bioadhesives have been used in surgery as hemostatic and wound healing agents. GRF (gelatin + resorcinol + formaldehyde) glue, composed of a mixture of gelatin and resorcinol polymerized by the addition of formaldehyde, has been used for this purpose. Widespread acceptance of the GRF glue, however, has been limited by reports of cytotoxicity due to its release of formaldehyde upon degradation. It has been suggested by Wertzel et al. that the cytotoxicity problem of GRF glue may be overcome by changing its cross-linking method. The study was, therefore, undertaken to assess the feasibility of using a water-soluble carbodiimide or genipin to cross-link gelatin as new bioadhesives to close skin wound lesions in a rat model. Formaldehyde-cross-linked counterpart (GRF glue) and a resorbable suture were used as controls. It was noted that the tensile strength of the skin across each wound treated by either application of test glues or suture increased consistently with time during the healing process. Also, the wounds repaired by test glues or suture caused no calcification. The suture used in the study was completely resorbed at the wound area in about 6 days postoperatively. However, the durations required to completely resorb the carbodiimide- or genipin-cross-linked glues were approximately the same (9 days), while it took about 14 days to completely resorb the formaldehyde-cross-linked glue. The healing process for the suture wound repaired was more rapid than those treated by test glues. Of the test glues, the wounds treated by the carbodiimide- or genipin-cross-linked glues induced less inflammatory response and recovered sooner than that treated by the formaldehyde-cross-linked glue. This indicated that the biocompatibility of the carbodiimide- or genipin-cross-linked glues was superior to the formaldehyde-cross-linked glue. The results of this study may serve as a preliminary experimental model for the further investigation of both the carbodiimide- and genipin-cross-linked glues when applied to human skin closure.

[1]  E. Khor Methods for the treatment of collagenous tissues for bioprostheses. , 1997, Biomaterials.

[2]  H. Sung,et al.  Feasibility study of a natural crosslinking reagent for biological tissue fixation. , 1998, Journal of biomedical materials research.

[3]  T. Iwashita,et al.  Structure of genipocyanin G1, a spontaneous reaction product between genipin and glycine , 1987 .

[4]  Y. Takeda,et al.  Studies on the Blue Pigments Produced from Genipin and Methylamine. I. Structures of the Brownish-Red Pigments, Intermediates Leading to the Blue Pigments , 1994 .

[5]  M. Higashiyama,et al.  Pneumostatic effect of gelatin-resorcinol formaldehyde-glutaraldehyde glue on thermal injury of the lung: an experimental study on rats. , 1997, European journal of cardio-thoracic surgery : official journal of the European Association for Cardio-thoracic Surgery.

[6]  H. Sung,et al.  In vitro evaluation of cytotoxicity of a naturally occurring cross-linking reagent for biological tissue fixation. , 1999, Journal of biomaterials science. Polymer edition.

[7]  Y. Ikada,et al.  In vitro evaluation of cytotoxicity of diepoxy compounds used for biomaterial modification. , 1995, Journal of biomedical materials research.

[8]  J. Cunningham,et al.  COMPARATIVE STUDY OF BIOLOGICAL GLUES. AUTHORS' REPLY , 1996 .

[9]  Y. Ikada,et al.  Rapidly curable biological glue composed of gelatin and poly(L-glutamic acid). , 1996, Biomaterials.

[10]  J. Feijen,et al.  Cross-linking of dermal sheep collagen using a water-soluble carbodiimide. , 1996, Biomaterials.

[11]  D. Lin,et al.  Crosslinking characteristics of an epoxy-fixed porcine tendon: effects of pH, temperature, and fixative concentration. , 1996, Journal of biomedical materials research.

[12]  D. Loisance,et al.  [Experimental test of two tissue adhesives (GRF and IBC 2) in vascular microsurgery in the rat (author's transl)]. , 1982, Journal de chirurgie.

[13]  K. Kobashi,et al.  Enzymic studies on the animal and intestinal bacterial metabolism of geniposide. , 1994, Biological & pharmaceutical bulletin.

[14]  Y. Ikada,et al.  A new biological glue from gelatin and poly (L-glutamic acid). , 1996, Journal of biomedical materials research.

[15]  Experimental gluing of lung parenchyma in rats. , 1997, The Thoracic and cardiovascular surgeon.

[16]  Y. Ikada,et al.  Macrophage activation through phagocytosis of muramyl dipeptide encapsulated in gelatin microspheres , 1987, The Journal of pharmacy and pharmacology.

[17]  J. Ennker,et al.  The impact of gelatin-resorcinol glue on aortic tissue: a histomorphologic evaluation. , 1994, Journal of vascular surgery.

[18]  R Vanholder,et al.  Cyanoacrylate tissue adhesive for closing skin wounds: a double blind randomized comparison with sutures. , 1993, Biomaterials.

[19]  Y. Ikada,et al.  Phagocytosis of Bioactive Microspheres , 1986 .

[20]  G. Teodori,et al.  Surgery of type A acute aortic dissection with Gelatine-Resorcine-Formol biological glue: a twelve-year experience. , 1990, The Journal of cardiovascular surgery.