The State of the Art in Machining Additively Manufactured Titanium Alloy Ti-6Al-4V
暂无分享,去创建一个
S. Ding | M. Mazur | G. Li | J. Mo | Chen Zhang | Dongyi Zou
[1] C. K. Nirala,et al. Measurement and analysis of tool wear and surface characteristics in micro turning of SLM Ti6Al4V and wrought Ti6Al4V , 2023, Measurement.
[2] Zhenhua Wang,et al. Effects of Heat Treatment on Sliding Wear and Milling Properties of Ti-6Al-4V Prepared by Selective Laser Melting , 2022, Journal of Tribology.
[3] B. C. Routara,et al. Study on machinability characteristics of novel additive manufactured titanium alloy (Ti-6Al-4V) fabricated by direct metal laser sintering , 2022, Proceedings of the Institution of Mechanical Engineers, Part C: Journal of Mechanical Engineering Science.
[4] A. Bandyopadhyay,et al. Role of porosity defects in metal 3D printing: Formation mechanisms, impacts on properties and mitigation strategies , 2022, Materials Today.
[5] I. Polozov,et al. Processing, Microstructure, and Mechanical Properties of Laser Additive Manufactured Ti2AlNb-Based Alloy with Carbon, Boron, and Yttrium Microalloying , 2022, Metals.
[6] A. Çiçek,et al. Machinability of 3D printed metallic materials fabricated by selective laser melting and electron beam melting: A review , 2022, Journal of Manufacturing Processes.
[7] E. Cerri,et al. Effect of surface roughness and industrial heat treatments on the microstructure and mechanical properties of Ti6Al4V alloy manufactured by laser powder bed fusion in different built orientations , 2022, Materials Science and Engineering: A.
[8] V. Jain,et al. State of the art on chemical and electrochemical based finishing processes for additive manufactured features , 2022, Additive Manufacturing.
[9] Lida Zhu,et al. Machining performance and wear mechanism of PVD TiAlN/AlCrN coated carbide tool in precision machining of selective laser melted Ti6Al4V alloys under dry and MQL conditions , 2022, Journal of Manufacturing Processes.
[10] Sajjad Ahmad,et al. Role of porosity in machinability of additively manufactured Ti-6Al-4V , 2022, Precision Engineering.
[11] C. Ventura,et al. Microstructural and machinability aspects of electron beam melted Ti–6Al–4V with different building orientations , 2022, Progress in Additive Manufacturing.
[12] S. Palanisamy,et al. Machinability Analysis of Finish-Turning Operations for Ti6Al4V Tubes Fabricated by Selective Laser Melting , 2022, Metals.
[13] D. Eliezer,et al. Corrosion behavior of AM-Ti-6Al-4V: a comparison between EBM and SLM , 2022, Progress in Additive Manufacturing.
[14] I. Jawahir,et al. Additive manufacturing of Ti-6Al-4V alloy- A review , 2022, Journal of Materials Research and Technology.
[15] A. Rollett,et al. Defects and anomalies in powder bed fusion metal additive manufacturing , 2022, Current Opinion in Solid State and Materials Science.
[16] J. Schoenung,et al. Laser-based directed energy deposition (DED-LB) of advanced materials , 2022, Materials Science and Engineering: A.
[17] Mengyao Zheng,et al. In-situ investigation of deformation behavior in additively manufactured FeCoCrNiMn high entropy alloy , 2022, Materials Science and Engineering: A.
[18] G. Wang,et al. Machinability performance and mechanism in milling of additive manufactured Ti6Al4V with polycrystalline diamond tool , 2022, Journal of Manufacturing Processes.
[19] S. Palanisamy,et al. Machinability of additively manufactured titanium alloys: A comprehensive review , 2022, Journal of Manufacturing Processes.
[20] R. Hellmann,et al. Tool Wear and Milling Characteristics for Hybrid Additive Manufacturing Combining Laser Powder Bed Fusion and In Situ High-Speed Milling , 2022, Materials.
[21] J. Raval,et al. Preliminary Study on Machining of Additively Manufactured Ti-6Al-4V , 2022, JOM.
[22] Yongsheng Su,et al. Surface integrity of ultrasonic-assisted dry milling of SLM Ti6Al4V using polycrystalline diamond tool , 2022, The International Journal of Advanced Manufacturing Technology.
[23] Guangping Guo,et al. Experimental studies on mechanical properties of laser powder bed fused Ti-6Al-4V alloy under post-heat treatment , 2022, Engineering Fracture Mechanics.
[24] Additive Manufacturing for Chemical Sciences and Engineering , 2022 .
[25] S. Bruschi,et al. Ball end milling machinability of additively and conventionally manufactured Ti6Al4V tilted surfaces , 2021, Journal of Manufacturing Processes.
[26] Ming Chen,et al. Microstructure- and cooling/lubrication environment-dependent machining responses in side milling of direct metal laser-sintered and rolled Ti6Al4V alloys , 2021, Journal of Materials Processing Technology.
[27] R. Hellmann,et al. Design Rules for Hybrid Additive Manufacturing Combining Selective Laser Melting and Micromilling , 2021, Materials.
[28] J. Seol,et al. Effects of Laser Power on the Microstructure Evolution and Mechanical Properties of Ti–6Al–4V Alloy Manufactured by Direct Energy Deposition , 2021, Metals and Materials International.
[29] Prashant Singh,et al. State-of-the-art in heat exchanger additive manufacturing , 2021 .
[30] R. R. Rahman Rashid,et al. Review on machining of additively manufactured nickel and titanium alloys , 2021, Journal of Materials Research and Technology.
[31] S. Ding,et al. A state-of-art review on chatter and geometric errors in thin-wall machining processes , 2021, Journal of Manufacturing Processes.
[32] Z. Xiao,et al. Improved surface integrity of Ti6Al4V fabricated by selective electron beam melting using ultrasonic surface rolling processing , 2021 .
[33] J. Schoenung,et al. Directed energy deposition (DED) additive manufacturing: Physical characteristics, defects, challenges and applications , 2021, Materials Today.
[34] S. Bruschi,et al. Turning of Additively Manufactured Ti6Al4V: Effect of the Highly Oriented Microstructure on the Surface Integrity , 2021, Materials.
[35] E. Zhao,et al. A comparative study on mechanical properties of Ti–6Al–4V alloy processed by additive manufacturing vs. traditional processing , 2021 .
[36] C. A. Vargas,et al. Additive manufacturing of Ti6Al4V alloy via electron beam melting for the development of implants for the biomedical industry , 2021, Heliyon.
[37] Y. Gong,et al. Mechanical performance of 316 L stainless steel by hybrid directed energy deposition and thermal milling process , 2021 .
[38] T. Ishimoto,et al. Unique crystallographic texture formation in Inconel 718 by laser powder bed fusion and its effect on mechanical anisotropy , 2021 .
[39] S. Palanisamy,et al. The Performance of Polycrystalline Diamond (PCD) Tools Machined by Abrasive Grinding and Electrical Discharge Grinding (EDG) in High-Speed Turning , 2021, Journal of Manufacturing and Materials Processing.
[40] A. Shahi,et al. Selective laser melting of Ti6Al4V alloy: Process parameters, defects and post-treatments , 2021 .
[41] G. Requena,et al. Separation of the impact of residual stress and microstructure on the fatigue performance of LPBF Ti-6Al-4V at elevated temperature , 2021, International Journal of Fatigue.
[42] Khamis Essa,et al. Powder-based laser hybrid additive manufacturing of metals: a review , 2021, The International Journal of Advanced Manufacturing Technology.
[43] R. Mohanraj,et al. Review on the evolution and technology of State-of-the-Art metal additive manufacturing processes , 2021 .
[44] A. Sarhan,et al. A Comprehensive Review on Machining of Titanium Alloys , 2021, Arabian Journal for Science and Engineering.
[45] D. Ahn. Directed Energy Deposition (DED) Process: State of the Art , 2021 .
[46] W. Haider,et al. Microstructural, corrosion and mechanical properties of additively manufactured alloys: a review , 2021, Critical Reviews in Solid State and Materials Sciences.
[47] M. Ramulu,et al. Mechanical anisotropy and its evolution with powder reuse in Electron Beam Melting AM of Ti6Al4V , 2021 .
[48] Guijian Xiao,et al. Multi-objective titanium alloy belt grinding parameters optimization oriented to resources allocation and environment , 2021, The International Journal of Advanced Manufacturing Technology.
[49] S. Bruschi,et al. Surface finish of additively manufactured Ti6Al4V workpieces after ball end milling , 2021, Procedia CIRP.
[50] V. Varghese,et al. Micromilling-induced Surface Integrity of Porous Additive Manufactured Ti6Al4V Alloy , 2021, Procedia Manufacturing.
[51] S. Bruschi,et al. Anisotropy effect of additively manufactured Ti6Al4V titanium alloy on surface quality after milling , 2021 .
[52] M. Bermingham,et al. Challenges in laser-assisted milling of titanium alloys , 2021, International Journal of Extreme Manufacturing.
[53] W. Matizamhuka,et al. Laser Powder Bed Fusion of Potential Superalloys: A Review , 2020, Metals.
[54] S. Kapoor,et al. The influence of additive manufacturing on the micromilling machinability of Ti6Al4V: A comparison of SLM and commercial workpieces , 2020 .
[55] A. Khan,et al. Tool wear, surface quality, and residual stresses analysis of micro-machined additive manufactured Ti–6Al–4V under dry and MQL conditions , 2020 .
[56] Chang-Bun Yoon,et al. Powder based additive manufacturing for biomedical application of titanium and its alloys: a review , 2020, Biomedical Engineering Letters.
[57] G. Manogharan,et al. Machining Behavior and Material Properties in Additive Manufacturing Ti-6Al-4V Parts , 2020 .
[58] K. Al-Rubaie,et al. Machinability of SLM-produced Ti6Al4V titanium alloy parts , 2020 .
[59] P. Hooper,et al. Study of the Effects of Hot Forging on the Additively Manufactured Stainless Steel Preforms , 2020 .
[60] A. Fatemi,et al. Defects in additive manufactured metals and their effect on fatigue performance: A state-of-the-art review , 2020 .
[61] S. Ding,et al. The manufacturing and the application of polycrystalline diamond tools – A comprehensive review , 2020 .
[62] S. Ding,et al. Machinablility of titanium matrix composites (TMC) reinforced with multi-walled carbon nanotubes , 2020 .
[63] Heng Zhang,et al. Cutting responses of additive manufactured Ti6Al4V with solid ceramic tool under dry high-speed milling processes , 2020 .
[64] J. Li,et al. Comparison study on microstructure and mechanical properties of Ti-6Al-4V alloys fabricated by powder-based selective-laser-melting and sintering methods , 2020 .
[65] A. Clare,et al. Machining of directed energy deposited Ti6Al4V using adaptive control , 2020, Journal of Manufacturing Processes.
[66] S. Bruschi,et al. Influence of additive manufacturing-induced anisotropy on tool wear in end milling of Ti6Al4V , 2020 .
[67] R. Boyer,et al. Opportunities and Issues in the Application of Titanium Alloys for Aerospace Components , 2020, Metals.
[68] Bi Zhang,et al. Experimental study on additive/subtractive hybrid manufacturing of 6511 steel: process optimization and machining characteristics , 2020, The International Journal of Advanced Manufacturing Technology.
[69] P. Wiśniewski,et al. Analysis of Microstructure and Properties of a Ti–AlN Composite Produced by Selective Laser Melting , 2020, Materials.
[70] Bi Zhang,et al. Effect of temperature buildup on milling forces in additive/subtractive hybrid manufacturing of Ti-6Al-4V , 2020 .
[71] Christoph Leyens,et al. Hybrid manufacturing of titanium Ti-6Al-4V combining laser metal deposition and cryogenic milling , 2020, The International Journal of Advanced Manufacturing Technology.
[72] Heng Zhang,et al. New observations on wear characteristics of solid Al2O3/Si3N4 ceramic tool in high speed milling of additive manufactured Ti6Al4V , 2020 .
[73] D. G. McCartney,et al. The Influence of Iron in Minimizing the Microstructural Anisotropy of Ti-6Al-4V Produced by Laser Powder-Bed Fusion , 2020, Metallurgical and Materials Transactions A.
[74] A. Fatemi,et al. Fatigue of additive manufactured Ti-6Al-4V, Part I: The effects of powder feedstock, manufacturing, and post-process conditions on the resulting microstructure and defects , 2020, International Journal of Fatigue.
[75] D. Biermann,et al. Study on machinability of additively manufactured and conventional titanium alloys in micro-milling process , 2020 .
[76] L. Thijs,et al. Increasing the productivity of laser powder bed fusion: Influence of the hull-bulk strategy on part quality, microstructure and mechanical performance of Ti-6Al-4V , 2020 .
[77] Dimitrios E. Manolakos,et al. A comparative investigation of Taguchi and full factorial design for machinability prediction in turning of a titanium alloy , 2020 .
[78] Yuanbo T. Tang,et al. On the size and orientation effect in additive manufactured Ti-6Al-4V , 2020 .
[79] S. Bruschi,et al. Effect of AM-induced Anisotropy on the Surface Integrity of Laser Powder Bed Fused Ti6Al4V Machined Parts , 2020, Procedia Manufacturing.
[80] H. Hamdi,et al. Analysis of the surface integrity induced by face milling of Laser Metal Deposited Ti-6Al-4V , 2020 .
[81] T. Özel,et al. Surface integrity induced in machining additively fabricated nickel alloy Inconel 625 , 2020 .
[82] E. Guglielmino,et al. Tensile and Creep Properties Improvement of Ti-6Al-4V Alloy Specimens Produced by Electron Beam Powder Bed Fusion Additive Manufacturing , 2019, Metals.
[83] Vinh Phu Nguyen,et al. The effects of material anisotropy on secondary processing of additively manufactured CoCrMo , 2019, Additive Manufacturing.
[84] Ming Chen,et al. Dynamic mechanical properties and machinability characteristics of selective laser melted and forged Ti6Al4V , 2019, Journal of Materials Processing Technology.
[85] S. Bruschi,et al. Improving surface integrity and corrosion resistance of additive manufactured Ti6Al4V alloy by cryogenic machining , 2019, The International Journal of Advanced Manufacturing Technology.
[86] Sachin V. Solanki,et al. Effects of graphene oxide nanofluids on cutting temperature and force in machining Ti-6Al-4V , 2019, The International Journal of Advanced Manufacturing Technology.
[87] Diana A. Lados,et al. Understanding the microstructure and mechanical properties of Ti-6Al-4V and Inconel 718 alloys manufactured by Laser Engineered Net Shaping , 2019, Additive Manufacturing.
[88] F. Walther,et al. Criticality of porosity defects on the fatigue performance of wire + arc additive manufactured titanium alloy , 2019, International Journal of Fatigue.
[89] Y. Shin,et al. Additive manufacturing of Ti6Al4V alloy: A review , 2019, Materials & Design.
[90] Steven Y. Liang,et al. A review of chatter vibration research in milling , 2019, Chinese Journal of Aeronautics.
[91] D. Wimpenny,et al. A critical evaluation of the microstructural gradient along the build direction in electron beam melted Ti-6Al-4V alloy , 2019, Materials Science and Engineering: A.
[92] Ż. A. Mierzejewska,et al. Mechanical Properties and Microstructure of DMLS Ti6Al4V Alloy Dedicated to Biomedical Applications , 2019, Materials.
[93] Adam T. Clare,et al. Machining of functionally graded Ti6Al4V/ WC produced by directed energy deposition , 2018, Additive Manufacturing.
[94] Simon Gaisford,et al. An Overview of 3D Printing Technologies for Soft Materials and Potential Opportunities for Lipid-based Drug Delivery Systems , 2018, Pharmaceutical Research.
[95] D. Umbrello,et al. Surface integrity of machined additively manufactured Ti alloys , 2018, Journal of Materials Processing Technology.
[96] S. Bruschi,et al. Surface Integrity Analysis of Ti6Al4V After Semi-finishing Turning Under Different Low-Temperature Cooling Strategies , 2018, Journal of Materials Engineering and Performance.
[97] Garret E. O’Donnell,et al. Optimisation of process parameters to address fundamental challenges during selective laser melting of Ti-6Al-4V: A review , 2018 .
[98] Bi Zhang,et al. Eddy current detection of subsurface defects for additive/subtractive hybrid manufacturing , 2018 .
[99] Fengzhou Fang,et al. State of the art of bioimplants manufacturing: part I , 2018 .
[100] M. Dargusch,et al. Effect of tool wear evolution on chip formation during dry machining of Ti-6Al-4V alloy , 2018 .
[101] Bi Zhang,et al. Machining characteristics of 18Ni-300 steel in additive/subtractive hybrid manufacturing , 2018 .
[102] S. Ding,et al. Investigation and modeling of flank wear process of different PCD tools in cutting titanium alloy Ti6Al4V , 2018 .
[103] Ehsan Malekipour,et al. Common defects and contributing parameters in powder bed fusion AM process and their classification for online monitoring and control: a review , 2018 .
[104] Thomas Duda,et al. 3D metal printing technology: the need to re-invent design practice , 2018, AI & SOCIETY.
[105] S. Melkote,et al. Milling of maraging steel components produced by selective laser melting , 2018 .
[106] Adam T. Clare,et al. On the machinability of directed energy deposited Ti6Al4V , 2018 .
[107] Z. Y. Liu,et al. Energy Consumption in Additive Manufacturing of Metal Parts , 2018 .
[108] J. Rech,et al. Influence of the finish cutting operations on the fatigue performance of Ti-6Al-4V parts produced by Selective Laser Melting , 2018 .
[109] Yuebin Guo,et al. Residual Stress in Metal Additive Manufacturing , 2018 .
[110] S. Bruschi,et al. Coupling machining and heat treatment to enhance the wear behaviour of an Additive Manufactured Ti6Al4V titanium alloy , 2017 .
[111] M. Goldberg,et al. A comparative study of mechanical properties and machinability of wrought and additive manufactured (selective laser melting) titanium alloy – Ti-6Al-4V , 2017 .
[112] R. Banerjee,et al. Additive manufacturing of metals: a brief review of the characteristic microstructures and properties of steels, Ti-6Al-4V and high-entropy alloys , 2017, Science and technology of advanced materials.
[113] Stefania Bruschi,et al. 3D finite element modelling of surface modification in dry and cryogenic machining of EBM Ti6Al4V alloy , 2017 .
[114] Young-Jin Kim,et al. Lasers in additive manufacturing: A review , 2017 .
[115] Wojciech Święszkowski,et al. Laser and Electron Beam Additive Manufacturing Methods of Fabricating Titanium Bone Implants , 2017 .
[116] W. Świȩszkowski,et al. Microstructure and mechanical properties investigation of CP titanium processed by selective laser melting (SLM) , 2017 .
[117] Peng Guo,et al. Study on microstructure, mechanical properties and machinability of efficiently additive manufactured AISI 316L stainless steel by high-power direct laser deposition , 2017 .
[118] Muzheng Xiao,et al. Study of hybrid additive manufacturing based on pulse laser wire depositing and milling , 2017 .
[119] C. Bowen,et al. Mechanical properties of titanium-based Ti–6Al–4V alloys manufactured by powder bed additive manufacture , 2017 .
[120] Stefania Bruschi,et al. Experimental investigation on the feasibility of dry and cryogenic machining as sustainable strategies when turning Ti6Al4V produced by Additive Manufacturing , 2017 .
[121] A. Chiba,et al. Effects of post-processing on cyclic fatigue response of a titanium alloy additively manufactured by electron beam melting , 2017 .
[122] S. Ding,et al. The prediction of cutting force in end milling titanium alloy (Ti6Al4V) with polycrystalline diamond tools , 2017 .
[123] Guy Littlefair,et al. Cutting force and surface finish analysis of machining additive manufactured titanium alloy Ti-6Al-4V , 2017 .
[124] M. Fischer,et al. Micro Cutting of Ti-6Al-4V Parts Produced by SLM Process , 2017 .
[125] S. Bruschi,et al. On the tool wear mechanisms in dry and cryogenic turning Additive Manufactured titanium alloys , 2017 .
[126] N. Hrabe,et al. Fatigue properties of a titanium alloy (Ti–6Al–4V) fabricated via electron beam melting (EBM): Effects of internal defects and residual stress , 2017 .
[127] Diana A. Lados,et al. Microstructure, static properties, and fatigue crack growth mechanisms in Ti-6Al-4V fabricated by additive manufacturing: LENS and EBM , 2016 .
[128] Q. Fang,et al. The effects of pore and second-phase particle on the mechanical properties of machining copper matrix from molecular dynamic simulation , 2016 .
[129] Stefania Bruschi,et al. Influence of the machining parameters and cooling strategies on the wear behavior of wrought and additive manufactured Ti6Al4V for biomedical applications , 2016 .
[130] C. Emmelmann,et al. Additive Manufacturing of Metals , 2016 .
[131] Guy Littlefair,et al. Tool Wear and Surface Integrity Analysis of Machined Heat Treated Selective Laser Melted Ti-6Al-4V , 2016 .
[132] A. Beese,et al. Review of Mechanical Properties of Ti-6Al-4V Made by Laser-Based Additive Manufacturing Using Powder Feedstock , 2016 .
[133] Wojciech Święszkowski,et al. Post Processing and Biological Evaluation of the Titanium Scaffolds for Bone Tissue Engineering , 2016, Materials.
[134] Olivier Rigo,et al. Electron beam melted Ti–6Al–4V: Microstructure, texture and mechanical behavior of the as-built and heat-treated material , 2016 .
[135] Ming-Wei Wu,et al. Anisotropy in the impact toughness of selective laser melted Ti–6Al–4V alloy , 2016 .
[136] Martin Leary,et al. The Influence of As-Built Surface Conditions on Mechanical Properties of Ti-6Al-4V Additively Manufactured by Selective Electron Beam Melting , 2016 .
[137] M. Goldberg,et al. Metallurgical and Machinability Characteristics of Wrought and Selective Laser Melted Ti-6Al-4V , 2016 .
[138] Standard Terminology for Additive Manufacturing – General Principles – Terminology , 2016 .
[139] L. Venkat Raghavan,et al. 3D Metal Printing Technology , 2016 .
[140] S. Bruschi,et al. The Influence of Material Properties on the Tool Crater Wear When Machining Ti6Al4 V Produced by Additive Manufacturing Technologies , 2016 .
[141] Ralf Schweizer,et al. Manufacturing Processes For Engineering Materials , 2016 .
[142] Stefania Bruschi,et al. Analysis of the Surface Integrity in Cryogenic Turning of Ti6Al4 V Produced by Direct Melting Laser Sintering , 2016 .
[143] Adam T. Clare,et al. Machining of additively manufactured parts: implications for surface integrity , 2016 .
[144] N. Shamsaei,et al. An overview of Direct Laser Deposition for additive manufacturing; Part I: Transport phenomena, modeling and diagnostics , 2015 .
[145] Galina Kasperovich,et al. Improvement of fatigue resistance and ductility of TiAl6V4 processed by selective laser melting , 2015 .
[146] Matthew S. Dargusch,et al. A new understanding of the wear processes during laser assisted milling 17-4 precipitation hardened stainless steel , 2015 .
[147] Stefania Bruschi,et al. Analysis of tool wear in cryogenic machining of additive manufactured Ti6Al4V alloy , 2015 .
[148] Todd Palmer,et al. Anisotropic tensile behavior of Ti-6Al-4V components fabricated with directed energy deposition additive manufacturing , 2015 .
[149] M. Bermingham,et al. Cutting force, chip formation, and tool wear during the laser-assisted machining a near-alpha titanium alloy BTi-6431S , 2015 .
[150] T. Becker,et al. HEAT TREATMENT OF TI-6 AL-4 V PRODUCED , 2015 .
[151] C. Tuck,et al. Effect of the build orientation on the mechanical properties and fracture modes of SLM Ti–6Al–4V , 2014 .
[152] Brent Stucker,et al. Analysis of defect generation in Ti–6Al–4V parts made using powder bed fusion additive manufacturing processes , 2014 .
[153] Francis H. Froes,et al. The Additive Manufacturing (AM) of Titanium Alloys , 2014 .
[154] Karen M. Taminger,et al. Integrated control of solidification microstructure and melt pool dimensions in electron beam wire feed additive manufacturing of Ti-6Al-4V , 2014 .
[155] Yung C. Shin,et al. Remanufacturing of turbine blades by laser direct deposition with its energy and environmental impact analysis , 2014 .
[156] S. Ding,et al. Thermal characteristics in milling Ti6Al4V with polycrystalline diamond tools , 2014, The International Journal of Advanced Manufacturing Technology.
[157] John P.T. Mo,et al. Thermal characteristics in milling Ti6Al4V with polycrystalline diamond tools , 2014 .
[158] William E. Frazier,et al. Metal Additive Manufacturing: A Review , 2014, Journal of Materials Engineering and Performance.
[159] S. Ding,et al. Experimental investigation of end milling of titanium alloys with polycrystalline diamond tools , 2014 .
[160] J. Paulo Davim,et al. Machining of titanium alloys , 2014 .
[161] Victor Songmene,et al. Machinability and Machining of Titanium Alloys: A Review , 2014 .
[162] P. Krishna,et al. An Experimental Investigation on Machinability Studies of Steels by Face Turning , 2014 .
[163] Riaz Muhammad,et al. Thermally enhanced ultrasonically assisted machining of Ti alloy , 2014 .
[164] Y. Rong,et al. PERFORMANCE OF A COATED CEMENTED CARBIDE TOOL IN HIGH SPEED MILLING OF TI-6AL-4V ALLOY , 2013 .
[165] Oscar Gonzalo,et al. Mechanisms involved in the improvement of Inconel 718 machinability by laser assisted machining (LAM) , 2013 .
[166] Martine Wevers,et al. Surface Roughness and Morphology Customization of Additive Manufactured Open Porous Ti6Al4V Structures , 2013, Materials.
[167] Moataz M. Attallah,et al. Microstructure and tensile properties of selectively laser-melted and of HIPed laser-melted Ti–6Al–4V , 2013 .
[168] B. Furet,et al. Degradation modes and tool wear mechanisms in finish and rough machining of Ti17 Titanium alloy under high-pressure water jet assistance , 2013 .
[169] Timothy P. Quinn,et al. Effects of processing on microstructure and mechanical properties of a titanium alloy (Ti–6Al–4V) fabricated using electron beam melting (EBM), Part 2: Energy input, orientation, and location , 2013 .
[170] H. Maier,et al. On the mechanical behaviour of titanium alloy TiAl6V4 manufactured by selective laser melting: Fatigue resistance and crack growth performance , 2013 .
[171] J. Davim,et al. REVIEW ON MACHINABILITY OF TITANIUM ALLOYS: THE PROCESS PERSPECTIVE , 2013 .
[172] J. Kruth,et al. Heat treatment of Ti6Al4V produced by Selective Laser Melting: Microstructure and mechanical properties , 2012 .
[173] M. Siddhpura,et al. A review of chatter vibration research in turning , 2012 .
[174] E. Brandl,et al. Microstructure of additive layer manufactured Ti–6Al–4V after exceptional post heat treatments , 2012 .
[175] R. Poprawe,et al. Laser additive manufacturing of metallic components: materials, processes and mechanisms , 2012 .
[176] Stephen C. Veldhuis,et al. Tool wear mechanisms and tool life enhancement in ultra-precision machining of titanium , 2012 .
[177] J. Davim. Machining of Metal Matrix Composites , 2012 .
[178] A. Paoletti,et al. Machinability Aspects of Metal Matrix Composites , 2012 .
[179] J. Ciurana,et al. Biomedical production of implants by additive electro-chemical and physical processes , 2012 .
[180] C. Veiga,et al. PROPERTIES AND APPLICATIONS OF TITANIUM ALLOYS: A BRIEF REVIEW , 2012 .
[181] Christoph Leyens,et al. Mechanical Properties of Additive Manufactured Ti-6Al-4V Using Wire and Powder Based Processes , 2011 .
[182] C. Colin,et al. As-Fabricated and Heat-Treated Microstructures of the Ti-6Al-4V Alloy Processed by Selective Laser Melting , 2011 .
[183] B. Baufeld,et al. Thermal expansion and lattice parameters of shaped metal deposited Ti–6Al–4V , 2011 .
[184] Bert Lauwers,et al. Surface Integrity in Hybrid Machining Processes , 2011 .
[185] Igor Smurov,et al. Surface Morphology in Selective Laser Melting of Metal Powders , 2011 .
[186] S. S. Al-Bermani,et al. The Origin of Microstructural Diversity, Texture, and Mechanical Properties in Electron Beam Melted Ti-6Al-4V , 2010 .
[187] M. Dargusch,et al. Thermally enhanced machining of hard-to-machine materials: a review , 2010 .
[188] Omer Van der Biest,et al. Texture and Crystal Orientation in Ti-6Al-4V Builds Fabricated by Shaped Metal Deposition , 2010 .
[189] B. Baufeld,et al. Additive manufacturing of Ti–6Al–4V components by shaped metal deposition: Microstructure and mechanical properties , 2010 .
[190] Ingomar Kelbassa,et al. Laser Additive Manufacturing , 2010 .
[191] Y. Shin,et al. Machinability improvement of titanium alloy (Ti–6Al–4V) via LAM and hybrid machining , 2010 .
[192] S. Palanisamy,et al. Effects of coolant pressure on chip formation while turning Ti6Al4V alloy , 2009 .
[193] M. Dargusch,et al. Characteristics of cutting forces and chip formation in machining of titanium alloys , 2009 .
[194] P. Arrazola,et al. Machinability of titanium alloys (Ti6Al4V and Ti555.3) , 2009 .
[195] Paul Mativenga,et al. Assessment of the machinability of Ti-6Al-4V alloy using the wear map approach , 2009 .
[196] L. Murr,et al. Microstructure and mechanical behavior of Ti-6Al-4V produced by rapid-layer manufacturing, for biomedical applications. , 2009, Journal of the mechanical behavior of biomedical materials.
[197] Anselmo Eduardo Diniz,et al. A comparison between silicon nitride-based ceramic and coated carbide tools in the face milling of irregular surfaces , 2008 .
[198] Claus Emmelmann,et al. Rapid manufacturing of lattice structures with selective laser melting , 2006, SPIE LASE.
[199] Songlin Ding,et al. Boundary-conformed machining of turbine blades , 2005 .
[200] M. A. Mannan,et al. Surface integrity when machining age hardened Inconel 718 with coated carbide cutting tools , 2004 .
[201] Carrie Bellnoski. A new understanding. , 2004, The Journal of neuroscience nursing : journal of the American Association of Neuroscience Nurses.
[202] Daniel C. H. Yang,et al. Boundary-conformed toolpath generation for trimmed free-form surfaces via Coons reparametrization , 2003 .
[203] S. L. Semiatin,et al. Microstructure and texture evolution during solidification processing of Ti–6Al–4V , 2003 .
[204] G. Lütjering,et al. Titanium Matrix Composites , 2003 .
[205] R. Komanduri,et al. On thermoplastic shear instability in the machining of a titanium alloy (Ti-6Al-4V) , 2002 .
[206] S. L. Semiatin,et al. The laser additive manufacture of Ti-6Al-4V , 2001 .
[207] G. Byrne,et al. Observations on chip formation and acoustic emission in machining Ti–6Al–4V alloy , 2001 .
[208] J. Jeng,et al. Mold fabrication and modification using hybrid processes of selective laser cladding and milling , 2001 .
[209] S. L. Semiatin,et al. The effect of laser power and traverse speed on microstructure, porosity, and build height in laser-deposited Ti-6Al-4V , 2000 .
[210] A. Jawaid,et al. Tool wear characteristics in turning of titanium alloy Ti-6246 , 1999 .
[211] Z. M. Wang,et al. Titanium alloys and their machinability—a review , 1997 .
[212] Herbert Schulz,et al. High-Speed Machining , 1992 .