Toward highly stable electrocatalysts via nanoparticle pore confinement.

The durability of electrode materials is a limiting parameter for many electrochemical energy conversion systems. In particular, electrocatalysts for the essential oxygen reduction reaction (ORR) present some of the most challenging instability issues shortening their practical lifetime. Here, we report a mesostructured graphitic carbon support, Hollow Graphitic Spheres (HGS) with a specific surface area exceeding 1000 m(2) g(-1) and precisely controlled pore structure, that was specifically developed to overcome the long-term catalyst degradation, while still sustaining high activity. The synthetic pathway leads to platinum nanoparticles of approximately 3 to 4 nm size encapsulated in the HGS pore structure that are stable at 850 °C and, more importantly, during simulated accelerated electrochemical aging. Moreover, the high stability of the cathode electrocatalyst is also retained in a fully assembled polymer electrolyte membrane fuel cell (PEMFC). Identical location scanning and scanning transmission electron microscopy (IL-SEM and IL-STEM) conclusively proved that during electrochemical cycling the encapsulation significantly suppresses detachment and agglomeration of Pt nanoparticles, two of the major degradation mechanisms in fuel cell catalysts of this particle size. Thus, beyond providing an improved electrocatalyst, this study describes the blueprint for targeted improvement of fuel cell catalysts by design of the carbon support.

[1]  A. Kostka,et al.  Stability investigations of electrocatalysts on the nanoscale , 2012 .

[2]  Ke Ke,et al.  An accurate evaluation for the activity of nano-sized electrocatalysts by a thin-film rotating disk electrode: Oxygen reduction on Pt/C , 2012 .

[3]  V. Stamenkovic,et al.  Advanced Platinum Alloy Electrocatalysts for the Oxygen Reduction Reaction , 2012 .

[4]  Thomas J. Schmidt,et al.  Electrocatalysis for Polymer Electrolyte Fuel Cells: Recent Achievements and Future Challenges , 2012 .

[5]  Yuyan Shao,et al.  Electrocatalysts for Nonaqueous Lithium–Air Batteries: Status, Challenges, and Perspective , 2012 .

[6]  A. Kostka,et al.  Degradation Mechanisms of Pt/C Fuel Cell Catalysts under Simulated Start–Stop Conditions , 2012 .

[7]  B. Popov,et al.  Electrocatalytic Activity and Stability of Titania-Supported Platinum–Palladium Electrocatalysts for Polymer Electrolyte Membrane Fuel Cell , 2012 .

[8]  Dustin Banham,et al.  First time investigation of Pt nanocatalysts deposited inside carbon mesopores of controlled length and diameter , 2012 .

[9]  Robert Hovden,et al.  Three-dimensional tracking and visualization of hundreds of Pt-Co fuel cell nanocatalysts during electrochemical aging. , 2012, Nano letters.

[10]  T. Nejat Veziroğlu,et al.  Polymer electrolyte fuel cell degradation , 2012 .

[11]  M. Arenz,et al.  The particle size effect on the oxygen reduction reaction activity of Pt catalysts: influence of electrolyte and relation to single crystal models. , 2011, Journal of the American Chemical Society.

[12]  N. Alonso‐Vante,et al.  Metal–Support Interactions between Nanosized Pt and Metal Oxides (WO3 and TiO2) Studied Using X-ray Photoelectron Spectroscopy , 2011 .

[13]  Yan-Jie Wang,et al.  Noncarbon support materials for polymer electrolyte membrane fuel cell electrocatalysts. , 2011, Chemical reviews.

[14]  Y. Liu,et al.  Electrocatalytic Activity and Stability of Pt clusters on State-of-the-Art Supports: A Review , 2011 .

[15]  T. Schmidt,et al.  Simulated start–stop as a rapid aging tool for polymer electrolyte fuel cell electrodes , 2011 .

[16]  Y. Shao-horn,et al.  Size Influence on the Oxygen Reduction Reaction Activity and Instability of Supported Pt Nanoparticles , 2011 .

[17]  P. Strasser,et al.  Activity, stability and degradation of multi walled carbon nanotube (MWCNT) supported Pt fuel cell electrocatalysts. , 2010, Physical chemistry chemical physics : PCCP.

[18]  M. Hickner,et al.  Uniform hollow carbon shells: nanostructured graphitic supports for improved oxygen-reduction catalysis. , 2010, Angewandte Chemie.

[19]  Wei Sheng Chen,et al.  Raman and X-ray diffraction analysis on unburned carbon powder refined from fly ash , 2010 .

[20]  B. Xia,et al.  Durability improvement of a Pt catalyst with the use of a graphitic carbon support. , 2010, Chemistry.

[21]  Michael F Toney,et al.  Lattice-strain control of the activity in dealloyed core-shell fuel cell catalysts. , 2010, Nature chemistry.

[22]  P. Atanassov,et al.  Templated Platinum/Carbon Oxygen Reduction Fuel Cell Electrocatalysts , 2010 .

[23]  Bertrand Lavédrine,et al.  Cover Picture: The Nature of the Extraordinary Finish of Stradivari’s Instruments (Angew. Chem. Int. Ed. 1/2010) , 2010 .

[24]  A S Bondarenko,et al.  Alloys of platinum and early transition metals as oxygen reduction electrocatalysts. , 2009, Nature chemistry.

[25]  P. Atanassov,et al.  Microparticles with bimodal nanoporosity derived by microemulsion templating. , 2009, Langmuir : the ACS journal of surfaces and colloids.

[26]  B. Fang,et al.  Hollow core/mesoporous shell carbon capsule as an unique cathode catalyst support in direct methanol fuel cell , 2009 .

[27]  H. Gasteiger,et al.  Just a Dream—or Future Reality? , 2009, Science.

[28]  Frédéric Jaouen,et al.  Iron-Based Catalysts with Improved Oxygen Reduction Activity in Polymer Electrolyte Fuel Cells , 2009, Science.

[29]  B. Fang,et al.  Hierarchical nanostructured hollow spherical carbon with mesoporous shell as a unique cathode catalyst support in proton exchange membrane fuel cell. , 2009, Physical chemistry chemical physics : PCCP.

[30]  Jong-Sung Yu,et al.  Ordered Hierarchical Nanostructured Carbon as a Highly Efficient Cathode Catalyst Support in Proton Exchange Membrane Fuel Cell , 2009 .

[31]  Sean James Ashton,et al.  Non-destructive transmission electron microscopy study of catalyst degradation under electrochemical treatment , 2008 .

[32]  Sean James Ashton,et al.  Fuel cell catalyst degradation on the nanoscale , 2008 .

[33]  Z. Lei,et al.  Graphitized carbon with hierarchical mesoporous structure templated from colloidal silica particles , 2008 .

[34]  Thomas J. Schmidt,et al.  Properties of high-temperature PEFC Celtec®-P 1000 MEAs in start/stop operation mode , 2008 .

[35]  Edward F. Holby,et al.  Instability of Supported Platinum Nanoparticles in Low-Temperature Fuel Cells , 2007 .

[36]  Geping Yin,et al.  Understanding and Approaches for the Durability Issues of Pt-Based Catalysts for PEM Fuel Cell , 2007 .

[37]  Mahlon Wilson,et al.  Scientific aspects of polymer electrolyte fuel cell durability and degradation. , 2007, Chemical reviews.

[38]  Philip N. Ross,et al.  Improved Oxygen Reduction Activity on Pt3Ni(111) via Increased Surface Site Availability , 2007, Science.

[39]  Hubert A. Gasteiger,et al.  The Impact of Carbon Stability on PEM Fuel Cell Startup and Shutdown Voltage Degradation , 2006 .

[40]  H. Tang,et al.  PEM fuel cell cathode carbon corrosion due to the formation of air/fuel boundary at the anode , 2006 .

[41]  I. Hsing,et al.  The effect of the Pt deposition method and the support on Pt dispersion on carbon nanotubes , 2006 .

[42]  A. B. Fuertes,et al.  Catalytic graphitization of templated mesoporous carbons , 2006 .

[43]  M. Arenz,et al.  CO surface electrochemistry on Pt-nanoparticles: A selective review , 2005 .

[44]  Jie Ding,et al.  Platinum and platinum-ruthenium nanoparticles supported on ordered mesoporous carbon and their electrocatalytic performance for fuel cell reactions , 2005 .

[45]  H. Gasteiger,et al.  Activity benchmarks and requirements for Pt, Pt-alloy, and non-Pt oxygen reduction catalysts for PEMFCs , 2005 .

[46]  A. B. Fuertes,et al.  Mesoporous carbons with graphitic structures fabricated by using porous silica materials as templates and iron-impregnated polypyrrole as precursor , 2005 .

[47]  F. Schüth Endo- and exotemplating to create high-surface-area inorganic materials. , 2003, Angewandte Chemie.

[48]  K. Tsutsumi,et al.  A Novel Pathway for Synthesis of Submicrometer‐Size Solid Core/Mesoporous Shell Silica Spheres , 1998 .

[49]  P. Buffat,et al.  Size effect on the melting temperature of gold particles , 1976 .

[50]  P. Stonehart,et al.  Potential cycling effects on platinum electrocatalyst surfaces , 1973 .