193-nm immersion lithography is the only choice for the 45-nm logical node at 120-nm half pitch and extendable to 32- and 22-nm nodes. The defect problem is one of the critical issues in immersion technology. In this paper, we provided a methodology to trace the defect source from optical microscope images to its SEM counterparts after exposure. An optimized exposure routing was also proposed to reduce printing defects. The average defect count was reduced from 19.7 to 4.8 ea/wafer.