Performance of metakaolin concrete at elevated temperatures
暂无分享,去创建一个
Salman Azhar | Chi Sun Poon | Y. L. Wong | M. Anson | C. Poon | S. Azhar | Y. Wong | Mike Anson
[1] Y. N. Chan,et al. Residual strength and pore structure of high-strength concrete and normal strength concrete after exposure to high temperatures , 1999 .
[2] J. P. Hurst,et al. Analytical Approach for Investigating the Causes of Spalling of High-Strength Concrete at Elevated Temperatures. , 1997 .
[3] J. Pera,et al. Pozzolanic activity of metakaolin under microwave treatment , 1995 .
[4] S. Wild,et al. Relative strength, pozzolanic activity and cement hydration in superplasticised metakaolin concrete , 1996 .
[5] M. Anson,et al. Fire Behavior of High-Performance Concrete Made with Silica Fume at Various Moisture Contents , 1999 .
[6] V. Penttala. EFFECTS OF MICROPOROSITY ON THE COMPRESSION STRENGTH AND FREEZING DURABILITY OF HIGH-STRENGTH CONCRETES , 1989 .
[7] G Sanjayan,et al. SPALLING OF HIGH-STRENGTH SILICA FUME CONCRETE IN FIRE , 1993 .
[8] G. Mohamedbhai. Effect of exposure time and rates of heating and cooling on residual strength of heated concrete , 1986 .
[9] Wei-Ming Lin,et al. Microstructures of Fire-Damaged Concrete , 1996 .