Blast Coating of Superelastic NiTi Wire with PTFE to Enhance Wear Properties

[1]  K. Stanton,et al.  Hydroxyapatite and fluorapatite coatings on dental screws: effects of blast coating process and biological response , 2015, Journal of Materials Science: Materials in Medicine.

[2]  K. Stanton,et al.  Co-blasting of titanium surfaces with an abrasive and hydroxyapatite to produce bioactive coatings: Substrate and coating characterisation , 2014, Journal of biomaterials applications.

[3]  P. McNally,et al.  Evaluation and comparison of hydroxyapatite coatings deposited using both thermal and non-thermal techniques , 2013 .

[4]  B. Twomey,et al.  Comparison between shot peening and abrasive blasting processes as deposition methods for hydroxyapatite coatings onto a titanium alloy , 2013 .

[5]  G. Cheng,et al.  Deformation Induced Martensite in NiTi and its Shape Memory Effects Generated by Low Temperature Laser Shock Peening , 2012 .

[6]  A. Crean,et al.  A Modified Surface on Titanium Deposited by a Blasting Process , 2011 .

[7]  A. Crean,et al.  Deposition of substituted apatites with anticolonizing properties onto titanium surfaces using a novel blasting process. , 2010, Journal of biomedical materials research. Part B, Applied biomaterials.

[8]  B. Meenan,et al.  Biological responses to hydroxyapatite surfaces deposited via a co-incident microblasting technique. , 2010, Biomaterials.

[9]  L. Sexton,et al.  Deposition of substituted apatites onto titanium surfaces using a novel blasting process , 2009 .

[10]  M. Peterlechner,et al.  Nanoscale amorphization of severely deformed NiTi shape memory alloys , 2009 .

[11]  A. Zieliński,et al.  Coatings in Arthroplasty: Review Paper , 2008 .

[12]  A. Amodeo,et al.  Comparative experimental evaluation of guidewire use in urology. , 2008, Urology.

[13]  Yinong Liu,et al.  Deformation-Induced Martensite Stabilisation in [1 0 0] Single-Crystalline Ni-Ti , 2006 .

[14]  T. Zhai,et al.  Enhancement of fatigue and corrosion properties of pure Ti by sandblasting , 2006 .

[15]  S. Kuribayashi,et al.  Lubrication performance of diamond-like carbon and fluorinated diamond-like carbon coatings for intravascular guidewires , 2006 .

[16]  T. Stolarski,et al.  Sliding performance of binary metal-PTFE coatings , 2004 .

[17]  Elspeth M McDougall,et al.  Comparison of guide wires in urology. Which, when and why? , 2004, The Journal of urology.

[18]  H. Maier,et al.  The effect of severe marforming on shape memory characteristics of a Ti-rich NiTi alloy processed using equal channel angular extrusion , 2003 .

[19]  Y. Mai,et al.  Laser shock processing and its effects on microstructure and properties of metal alloys: a review , 2002 .

[20]  M. Es‐Souni,et al.  On the properties of two binary NiTi shape memory alloys. Effects of surface finish on the corrosion behaviour and in vitro biocompatibility. , 2002, Biomaterials.

[21]  Swee Hin Teoh,et al.  Fatigue of biomaterials: a review , 2000 .

[22]  P. Prevéy X-ray diffraction characterization of crystallinity and phase composition in plasma-sprayed hydroxyapatite coatings , 2000 .

[23]  C. Doyle,et al.  Plasma sprayed hydroxyapatite coatings on titanium substrates. Part 2: optimisation of coating properties. , 1998, Biomaterials.

[24]  F. Haider,et al.  The role of the martensite transformation for the mechanical amorphisation of NiTi , 1997 .

[25]  Sarah Green,et al.  The surface performance of shot peened and ion implanted NiTi shape memory alloy , 1995 .

[26]  R. E. Jensen,et al.  Loss of hydroxyapatite coating on retrieved, total hip components. , 1993, The Journal of arthroplasty.

[27]  S. K. Biswas,et al.  Friction and wear of PTFE — a review , 1992 .

[28]  S D Cook,et al.  Experimental coating defects in hydroxylapatite-coated implants. , 1991, Clinical orthopaedics and related research.

[29]  D. Parkin,et al.  Crystal-to-amorphous transformation of NiTi induced by cold rolling , 1990 .