Reaction Mechanism and Microstructure Development of Zr–Si Alloyed Melt‐Infiltrated ZrC‐Modified C/C Composite

This work is supported by the National Natural Science Foundation of China(51302315), the Innovation Foundation for Excellent Postgraduate of NationalUniversity of Defense Technology, and the Hunan Provincial InnovationFoundation for Postgraduate. Yonggang Tong also thanks the support fromChina Scholarship Council.

[1]  H. Hu,et al.  Influence of pyrocarbon amount in C/C preform on the microstructure and properties of C/ZrC composites prepared via reactive melt infiltration , 2014 .

[2]  Hejun Li,et al.  Microstructure and oxidation resistance of Si–Mo–B coating for C/SiC coated carbon/carbon composites , 2013 .

[3]  Yu Zhou,et al.  Influence of reactive melt infiltration parameters on microstructure and properties of low temperature derived Cf/ZrC composites , 2013 .

[4]  Wei Sun,et al.  Microstructure and ablation behavior of carbon/carbon composites infiltrated with Zr–Ti , 2013 .

[5]  H. Hu,et al.  Mechanism of ablation of 3D C/ZrC–SiC composite under an oxyacetylene flame , 2013 .

[6]  Song Wang,et al.  Preparation of carbon fiber-reinforced zirconium carbide matrix composites by reactive melt infiltration at relative low temperature , 2012 .

[7]  S. Bai,et al.  C/C–ZrC composite prepared by chemical vapor infiltration combined with alloyed reactive melt infiltration , 2012 .

[8]  H. Hu,et al.  Ablation behavior and mechanism of 3D C/ZrC composite in oxyacetylene torch environment , 2011 .

[9]  Lai-fei Cheng,et al.  Reaction kinetics and ablation properties of C/C–ZrC composites fabricated by reactive melt infiltration , 2011 .

[10]  Hejun Li,et al.  Ablation of the carbon/carbon composite nozzle-throats in a small solid rocket motor , 2011 .

[11]  William E Lee,et al.  Reactive infiltration processing (RIP) of ultra high temperature ceramics (UHTC) into porous C/C composite tubes , 2011 .

[12]  Jenn‐Ming Yang,et al.  Microstructural development of a Cf/ZrC composite manufactured by reactive melt infiltration , 2010 .

[13]  Li Kezhi,et al.  Microstructure and ablation properties of zirconium carbide doped carbon/carbon composites , 2010 .

[14]  Anilesh Kumar,et al.  Capillary infiltration studies of liquids into 3D-stitched C–C preforms: Part B: Kinetics of silicon infiltration , 2009 .

[15]  Song Wang,et al.  Thermodynamic assessment of the C–Si–Zr system , 2009 .

[16]  Ke Yang,et al.  Ablation behaviors of ultra-high temperature ceramic composites , 2007 .

[17]  Q. Guo,et al.  Resistance to ablation of pitch-derived ZrC/C composites , 2004 .

[18]  M. Ferraris,et al.  Oxidation protective multilayer coatings for carbon-carbon composites , 2002 .

[19]  Jonathan A. Salem,et al.  Evaluation of ultra-high temperature ceramics foraeropropulsion use , 2002 .

[20]  Richard J. Day,et al.  Oxidation protection for carbon fibre composites , 1996, Journal of Materials Science.

[21]  J. Sheehan Oxidation protection for carbon fiber composites , 1989 .

[22]  J. Tobin,et al.  Kinetics of the zirconium--carbon reaction at temperatures above 2000$sup 0$C , 1965 .