Long-Term Water Balance Evaluation in Glass Ionomer Restorative Materials

The complex role of water in glass ionomer cement (polyalkenoate) dental restorative materials has been studied, but much of the present understanding concerning water balance within these materials is based on very early studies and short-term experiments. This study evaluated the nature of the water species of six conventional and four resin modified glass ionomer restorative materials over 3 years using thermogravimetric analysis techniques. Materials were prepared, placed in crucibles, and stored in physiologic phosphate buffered saline and evaluated at 24 h, 1 week, and then at 1, 3, 6, 9, 12, 18, 24, 30 and 36 months. All materials demonstrated a significant increase in unbound water percentage content but except for the resin modified materials, the enthalpy required to remove the unbound water species did not significantly change over 36 months. Also, bound water content percentage and removal enthalpy was established at 24 h, as no significant increase was noted in both bound water content and removal enthalpy over the course of this evaluation. This study suggests that unbound water species may increase with time and is loosely held except for the resin modified materials. Protective coatings placement and re-evaluation are prudent to prevent unbound water loss.

[1]  O. Erdem,et al.  Investigation of water sorption and aluminum releases from high viscosity and resin modified glass ionomer , 2020, Journal of clinical and experimental dentistry.

[2]  B. Czarnecka,et al.  Enhancing the Mechanical Properties of Glass-Ionomer Dental Cements: A Review , 2020, Materials.

[3]  S. Parker,et al.  Polymerization shrinkage kinetics and degree of conversion of commercial and experimental resin modified glass ionomer luting cements (RMGICs). , 2020, Dental materials : official publication of the Academy of Dental Materials.

[4]  R. Hickel,et al.  Six-year results of a randomized controlled clinical trial of two glass ionomer cements in class II cavities. , 2020, Journal of dentistry.

[5]  I. Miletić,et al.  Clinical Performance of a Glass-Hybrid System Compared with a Resin Composite in the Posterior Region: Results of a 2-year Multicenter Study. , 2020, The journal of adhesive dentistry.

[6]  E. Ergin,et al.  A randomized controlled 10 years follow up of a glass ionomer restorative material in class I and class II cavities. , 2020, Journal of dentistry.

[7]  G. McKenna,et al.  An RCT of atraumatic restorative treatment for older adults: 5 year results. , 2019, Journal of dentistry.

[8]  J. Nicholson,et al.  The effect of antimicrobial additives on the properties of dental glass-ionomer cements: a review , 2019, Acta biomaterialia odontologica Scandinavica.

[9]  L. Torre,et al.  Biological, thermal and mechanical characterization of modified glass ionomer cements: The role of nanohydroxyapatite, ciprofloxacin and zinc l-carnosine. , 2019, Materials science & engineering. C, Materials for biological applications.

[10]  J. Frencken,et al.  Survival percentages of atraumatic restorative treatment (ART) restorations and sealants in posterior teeth: an updated systematic review and meta-analysis , 2018, Clinical Oral Investigations.

[11]  L. Daemen,et al.  Nanoscale Mobility of Aqueous Polyacrylic Acid in Dental Restorative Cements. , 2018, ACS applied materials & interfaces.

[12]  J. Nicholson Maturation processes in glass-ionomer dental cements , 2018, Acta biomaterialia odontologica Scandinavica.

[13]  T. Seydel,et al.  Water dynamics in glass ionomer cements , 2016 .

[14]  Muhammad Sohail Zafar,et al.  Modifications in Glass Ionomer Cements: Nano-Sized Fillers and Bioactive Nanoceramics , 2016, International journal of molecular sciences.

[15]  C. Zelmer,et al.  Synthesis and characterization of POSS-(PAA)8 star copolymers and GICs for dental applications. , 2016, Dental materials : official publication of the Academy of Dental Materials.

[16]  B. Czarnecka,et al.  The effect of petroleum jelly, light-cured varnish and different storage media on the flexural strength of glass ionomer dental cements , 2016, Acta biomaterialia odontologica Scandinavica.

[17]  B. Czarnecka,et al.  THE EFFECT OF IONIC SOLUTIONS ON THE UPTAKE AND WATER-BINDING BEHAVIOUR OF GLASS-IONOMER DENTAL CEMENTS , 2016 .

[18]  L. Pavić,et al.  New Insights into the Setting Processes of Glass Ionomer Cements from Analysis of Dielectric Properties , 2015 .

[19]  Y. K. Kim,et al.  Setting Reaction of Dental Resin-Modified Glass Ionomer Restoratives as a Function of Curing Depth and Postirradiation Time , 2015 .

[20]  G. Fleming,et al.  Conventional glass-ionomer materials: A review of the developments in glass powder, polyacid liquid and the strategies of reinforcement. , 2015, Journal of dentistry.

[21]  Y. Yue,et al.  Phase separation in an ionomer glass: Insight from calorimetry and phase transitions , 2015 .

[22]  D. Berzins,et al.  Early reaction kinetics of contemporary glass-ionomer restorative materials. , 2015, The journal of adhesive dentistry.

[23]  D. Berzins,et al.  Thermal analysis of contemporary glass-ionomer restorative materials , 2014, Journal of Thermal Analysis and Calorimetry.

[24]  M. Khoroushi,et al.  A review of glass-ionomers: From conventional glass-ionomer to bioactive glass-ionomer , 2013, Dental research journal.

[25]  J. Frencken,et al.  Twenty-five-year atraumatic restorative treatment (ART) approach: a comprehensive overview , 2012, Clinical Oral Investigations.

[26]  M. Towler,et al.  A spectroscopic investigation into the setting and mechanical properties of titanium containing glass polyalkenoate cements , 2010, Journal of materials science. Materials in medicine.

[27]  G. Spoto,et al.  Thermal analysis of light-curing composites , 2010 .

[28]  R. Hand,et al.  Surface hydration and nanoindentation of silicate glasses , 2010 .

[29]  C. A. Wilkie,et al.  Resin-modified Glass-ionomer Setting Reaction Competition , 2010, Journal of dental research.

[30]  N. Zainuddin,et al.  A long-term study on the setting reaction of glass ionomer cements by (27)Al MAS-NMR spectroscopy. , 2009, Dental materials : official publication of the Academy of Dental Materials.

[31]  B. Darvell,et al.  Network competition in a resin-modified glass-ionomer cement. , 2008, Dental materials : official publication of the Academy of Dental Materials.

[32]  B. Czarnecka,et al.  Kinetic studies of water uptake and loss in glass-ionomer cements , 2008, Journal of materials science. Materials in medicine.

[33]  P. Hornsby Dimensional stability of glass‐ionomer cements , 2007 .

[34]  Alan D. Wilson,et al.  The glass‐ionomer cement, a new translucent dental filling material , 2007 .

[35]  Alan D. Wilson,et al.  Litho‐ionomer cements and their technological applications , 2007 .

[36]  P. Lambrechts,et al.  Glass-ionomer adhesion: The mechanisms at the interface , 2006 .

[37]  R. Hill,et al.  MAS-NMR spectroscopy studies in the setting reaction of glass ionomer cements. , 2006, Journal of dentistry.

[38]  F. Micelli,et al.  Characterization of the kinetic behavior of resin modified Glass-ionomer cements by DSC, TMA and ultrasonic wave propagation , 2001, Journal of materials science. Materials in medicine.

[39]  P. Jevnikar,et al.  Effect of surface coating on water migration into resin‐modified glass ionomer cements: A magnetic resonance micro‐imaging study , 2000, Magnetic resonance in medicine.

[40]  A. Young,et al.  Use of Raman spectroscopy in the characterisation of the acid-base reaction in glass-ionomer cements. , 2000, Biomaterials.

[41]  G. Cardenas,et al.  Thermal properties and TGA–FTIR studies of polyacrylic and polymethacrylic acid doped with metal clusters , 2000 .

[42]  A. Akamine,et al.  The relationship between water absorption characteristics and the mechanical strength of resin-modified glass-ionomer cements in long-term water storage. , 1999, Biomaterials.

[43]  A. Wan,et al.  Acid-base complex reactions in resin-modified and conventional glass ionomer cements. , 1999, Journal of biomedical materials research.

[44]  E. Atkins,et al.  Investigation of glass–ionomer cements using differential scanning calorimetry , 1998, Journal of materials science. Materials in medicine.

[45]  J. Nicholson,et al.  Chemistry of glass-ionomer cements: a review. , 1998, Biomaterials.

[46]  S. Matsuya,et al.  IR and NMR Analyses of Hardening and Maturation of Glass-ionomer Cement , 1996, Journal of dental research.

[47]  M. Miyazaki,et al.  Effect of surface coatings on flexural properties of glass ionomers. , 1996, European journal of oral sciences.

[48]  A. Kakaboura,et al.  An FTIR study on the setting mechanism of resin-modified glass ionomer restoratives. , 1996, Dental materials : official publication of the Academy of Dental Materials.

[49]  J. Nicholson,et al.  Studies in the setting of polyelectrolyte materials , 1995 .

[50]  A. Feilzer,et al.  The influence of water sorption on the development of setting shrinkage stress in traditional and resin-modified glass ionomer cements. , 1995, Dental materials : official publication of the Academy of Dental Materials.

[51]  K. Hiller,et al.  Influence of different factors on bond strength of hybrid ionomers. , 1995, Operative dentistry.

[52]  J. McCabe,et al.  Factors that influence the setting characteristics of encapsulated glass ionomer cements. , 1994, Journal of dentistry.

[53]  J. Meyer,et al.  Mechanical behavior of glass ionomer cements affected by long-term storage in water. , 1994, Dental materials : official publication of the Academy of Dental Materials.

[54]  P. Hatton,et al.  Characterisation of the ultrastructure of glass-ionomer (poly-alkenoate) cement , 1992, British Dental Journal.

[55]  J. McCabe,et al.  Light-activated glass polyalkenoate (ionomer) cements: the setting reaction. , 1992, Journal of dentistry.

[56]  H. Hirukawa,et al.  Effect of coating materials on restorative glass-ionomer cement surface. , 1992, Operative dentistry.

[57]  S. Mitra Adhesion to Dentin and Physical Properties of a Light-cured Glass-ionomer Liner/Base , 1991, Journal of dental research.

[58]  I. C. Mcneill,et al.  Thermal stability and degradation mechanisms of poly(acrylic acid) and its salts: Part 3—Magnesium and calcium salts , 1990 .

[59]  I. C. Mcneill,et al.  Thermal stability and degradation mechanisms of poly(acrylic acid) and its salts: Part 1—Poly(acrylic acid) , 1990 .

[60]  Alan D. Wilson,et al.  Thermal behaviour of films of partially neutralized poly(acrylic acid). 3: Effect of magnesium and calcium ions , 1988 .

[61]  Alan D. Wilson,et al.  Thermal behaviour of films of partially neutralized poly(acrylic acid). 1: Influence of metal ions , 1987 .

[62]  Alan D. Wilson,et al.  The hydration of a glass‐ionomer (ASPA) cement , 1981 .

[63]  A. D. Wilson,et al.  Dental Silicate Cements: XII. The Role of Water , 1970, Journal of dental research.

[64]  A. D. Wilson,et al.  Dental Silicate Cements. I. The Chemistry of Erosion , 1967, Journal of dental research.