Microstructure and ablation properties of La2O3 modified C/C-SiC composites prepared via precursor infiltration pyrolysis
暂无分享,去创建一个
K. He | Qizhong Huang | Lei Chen | Xin Yang | Cunqian Fang | Guang Zeng | Anhong Shi | Boyun Huang
[1] Hejun Li,et al. Long-time ablation protection of carbon/carbon composites with different-La2O3-content modified ZrC coating , 2017 .
[2] Brian Thompson,et al. Effect of rare-earth dopant (Sm) concentration on total hemispherical emissivity and ablation resistance of ZrB2/SiC coatings , 2016 .
[3] Hejun Li,et al. Ablation behavior of ZrC-La2O3 coating for SiC-coated carbon/carbon composites under an oxyacetylene torch , 2016 .
[4] Xue Feng,et al. Formation mechanisms of characteristic structures on the surface of C/SiC composites subjected to thermal ablation , 2016 .
[5] Yiguang Wang,et al. Multiple ablation resistance of La2O3/Y2O3-doped C/SiC–ZrC composites , 2015 .
[6] Liping Wang,et al. Fabrication and ablation property of carbon/carbon composites with novel SiC-ZrB2 coating , 2015 .
[7] Qizhong Huang,et al. Preparation of a double layer SiC coating and its oxidation resistance at 1773 K , 2014 .
[8] Aijun Li,et al. Microstructure and ablation mechanism of C/C–SiC composites , 2014 .
[9] Qizhong Huang,et al. Microstructure and ablation behavior of SiC coated C/C–SiC–ZrC composites prepared by a hybrid infiltration process , 2013 .
[10] F. Qin,et al. Oxidation kinetics and mechanisms of four-direction carbon/carbon composites and their components in carbon dioxide at high temperature , 2013 .
[11] A. Ohtomo,et al. Improved visible light driven photoelectrochemical properties of 3C-SiC semiconductor with Pt nanoparticles for hydrogen generation , 2013 .
[12] L. Chai,et al. Resistance to oxidation and ablation of SiC coating on graphite prepared by chemical vapor reaction , 2013 .
[13] Wei Sun,et al. Microstructure and ablation behavior of carbon/carbon composites infiltrated with Zr–Ti , 2013 .
[14] T. Asaka,et al. Thermal expansion of lanthanum silicate oxyapatite (La9.33+2x(SiO4)6O2+3x), lanthanum oxyorthosilicate (La2SiO5) and lanthanum sorosilicate (La2Si2O7) , 2012 .
[15] Yu-Lin Kuo,et al. Assessment of thermochemically stable apatite La10(SiO4)6O3 as electrolyte for solid oxide fuel cells , 2012 .
[16] K. Enya,et al. High-precision CTE measurement of hybrid C/SiC composite for cryogenic space telescopes , 2011, 1110.2620.
[17] Wenya Li,et al. Electrical Properties of Atmospheric Plasma-Sprayed La10(SiO4)6O3 Electrolyte Coatings , 2011 .
[18] Hejun Li,et al. Microstructure and oxidation of multi-layer MoSi2–CrSi2–Si coatings for SiC coated carbon/carbon composites , 2010 .
[19] J. Chessa,et al. An Evaluation of Vaporizing Rates of SiO2 and TiO2 As Protective Coatings for Ultrahigh Temperature Ceramic Composites , 2008 .
[20] Jiecai Han,et al. The addition of lanthanum hexaboride to zirconium diboride for improved oxidation resistance , 2007 .
[21] S. Mentus,et al. Lanthanum nitrate decomposition by both temperature programmed heating and citrate gel combustion , 2007 .
[22] K. Fukuda,et al. Crystal structure of lanthanum oxyorthosilicate, La2SiO5 , 2006, Powder Diffraction.
[23] Xiaohong Shi,et al. Silicon carbide coating to protect carbon/carbon composites against oxidation , 2005 .
[24] Stephan Schmidt,et al. Advanced ceramic matrix composite materials for current and future propulsion technology applications , 2004 .
[25] M. Fleet,et al. High-pressure synthesis of a La orthosilicate and Nd, Gd, and Dy disilicates , 2002 .
[26] R. Day,et al. Conversion of polycarbosilane (PCS) to SiC-based ceramic Part II Pyrolysis and characterisation , 2001 .
[27] G. Tzvetkov,et al. Mechanochemically induced formation of La2SiO5 , 2000 .
[28] G. Tzvetkov,et al. Application of mechanochemical treatment to the synthesis of A-and G-forms of La2Si2O7 , 1999 .
[29] N. Imanaka,et al. The Binary Rare Earth Oxides. , 1998, Chemical reviews.
[30] H. Seifert,et al. The Identity of Monoclinic La2O3 and Monoclinic Pr2O3 with La9.33(SiO4)6O2 and Pr9.33(SiO4)6O2, Respectively , 1995 .
[31] T. Cooke. Inorganic Fibers—A Literature Review , 1991 .
[32] G. W. Pearsall,et al. Frictional Boundary Conditions in Plastic Compression , 1963 .
[33] P. N. Walsh,et al. RARE EARTHS. I. VAPORIZATION OF La2O3 AND Nd2O3: DISSOCIATION ENERGIES OF GASEOUS LaO AND NdO1 , 1961 .