Kinetics of the water-gas shift reaction on Pt catalysts supported on alumina and ceria

Abstract We report the kinetic parameters for the water–gas shift (WGS) reaction on Pt catalysts supported on ceria and alumina under fuel reformer conditions for fuel cell applications (6.8% CO, 8.5% CO2, 22% H2O, 37.3% H2, and 25.4% Ar) at a total pressure of 1 atm and in the temperature range of 180–345 °C. When ceria was used as a support, the turnover rate (TOR) for WGS was 30 times that on alumina supported Pt catalysts. The overall WGS reaction rate (r) on Pt/alumina catalysts as a function of the forward rate (rf) was found to be: r = rf(1 − β), where rf = kf[CO]0.1[H2O]1.0[CO2]−0.1[H2]−0.5, kf is the forward rate constant, β = ([CO2][H2])/(Keq[CO][H2O]) is the approach to equilibrium, and Keq is the equilibrium constant for the WGS reaction. The negative apparent reaction orders indicate inhibition of the forward rate by CO2 and H2. The surface is saturated with CO on Pt under reaction conditions as confirmed by diffuse reflectance infrared Fourier transform spectroscopy (DRIFTS). The small positive apparent reaction order for CO, in concert with the negative order for H2 and the high CO coverage is explained by a decrease in the heat of adsorption as the CO coverage increases. Kinetic models based on redox-type mechanisms can explain the observed reaction kinetics and can qualitatively predict the changes in CO coverage observed in the DRIFTS study.

[1]  Raymond J. Gorte,et al.  Studies of the water-gas-shift reaction on ceria-supported Pt, Pd, and Rh: Implications for oxygen-storage properties , 1998 .

[2]  Manos Mavrikakis,et al.  Prediction of Experimental Methanol Decomposition Rates on Platinum from First Principles , 2006 .

[3]  T. Shido,et al.  Regulation of reaction intermediate by reactant in the water-gas shift reaction on CeO2, in relation to reactant-promoted mechanism , 1992 .

[4]  Michel Boudart,et al.  Kinetics of Heterogeneous Catalytic Reactions , 1984 .

[5]  G. Jacobs,et al.  Water-gas shift catalysis: kinetic isotope effect identifies surface formates in rate limiting step for Pt/ceria catalysts , 2004 .

[6]  Dionisios G. Vlachos,et al.  Microkinetic Modeling for Water-Promoted CO Oxidation, Water−Gas Shift, and Preferential Oxidation of CO on Pt , 2004 .

[7]  W. Nicholas Delgass,et al.  Spectroscopy in Heterogeneous Catalysis , 1979 .

[8]  S. Tsang,et al.  Engineering Pt in ceria for a maximum metal-support interaction in catalysis. , 2005, Journal of the American Chemical Society.

[9]  D. Bianchi,et al.  Heat of Adsorption of Carbon Monoxide on a Pt/Rh/CeO2/Al2O3Three-Way Catalyst Usingin-SituInfrared Spectroscopy at High Temperatures , 1998 .

[10]  D. Duprez,et al.  Steam effects in three-way catalysis , 1994 .

[11]  Robert J. Farrauto,et al.  NEW MATERIAL NEEDS FOR HYDROCARBON FUEL PROCESSING: Generating Hydrogen for , 2003 .

[12]  Manos Mavrikakis,et al.  Why Au and Cu Are More Selective Than Pt for Preferential Oxidation of CO at Low Temperature , 2004 .

[13]  R. Zapf,et al.  Water-gas shift reaction in micro-channels—Results from catalyst screening and optimisation , 2005 .

[14]  Robert J. Farrauto,et al.  Determination of kinetic parameters for the water-gas shift reaction on copper catalysts under realistic conditions for fuel cell applications , 2003 .

[15]  M. Flytzani-Stephanopoulos,et al.  Active Nonmetallic Au and Pt Species on Ceria-Based Water-Gas Shift Catalysts , 2003, Science.

[16]  Douglas C. Montgomery,et al.  Applied Statistics and Probability for Engineers, Third edition , 1994 .

[17]  R. Radhakrishnan,et al.  Water gas shift activity and kinetics of Pt/Re catalysts supported on ceria-zirconia oxides , 2006 .

[18]  Manos Mavrikakis,et al.  Molecular-level descriptions of surface chemistry in kinetic models using density functional theory , 2004 .

[19]  L. Schmidt,et al.  Binding states of CO on single crystal planes of Pt , 1977 .

[20]  Hans Bohlbro,et al.  An investigation on the kinetics of the conversion of carbon monoxide with water vapour over iron oxide based catalysts , 1969 .

[21]  J. M. Zalc,et al.  Are Noble Metal-Based Water–Gas Shift Catalysts Practical for Automotive Fuel Processing? , 2002 .

[22]  T. Shido,et al.  Reactant-Promoted Reaction Mechanism for Water-Gas Shift Reaction on Rh-Doped CeO2 , 1993 .

[23]  M. Mavrikakis,et al.  Lattice strain effects on CO oxidation on Pt(111). , 2006, Physical chemistry chemical physics : PCCP.

[24]  C. Lund Microkinetics of Water−Gas Shift over Sulfided Mo/Al2O3 Catalysts , 1996 .

[25]  P Hu,et al.  Catalytic water formation on platinum: a first-principles study. , 2001, Journal of the American Chemical Society.

[26]  I. Barin Thermochemical data of pure substances , 1989 .

[27]  Robert J. Farrauto,et al.  Mechanism of aging for a Pt/CeO2-ZrO2 water gas shift catalyst , 2006 .

[28]  Warren E. Stewart,et al.  Parameter estimation from multiresponse data , 1992 .

[29]  J. E. Benson,et al.  Hydrogen-oxygen titration method for the measurement of supported palladium surface areas , 1965 .

[30]  A. Ghenciu,et al.  Study of the origin of the deactivation of a Pt/CeO2 catalyst during reverse water gas shift (RWGS) reaction , 2004 .

[31]  Ib Chorkendorff,et al.  A Microkinetic Analysis of the Water–Gas Shift Reaction under Industrial Conditions , 1996 .

[32]  Charles T. Campbell,et al.  A kinetic model of the water gas shift reaction , 1992 .

[33]  J. Lunsford,et al.  The catalytic reactions of CO and H2O over supported rhodium , 1982 .

[34]  Jun Yi,et al.  CO2-reforming of methane on transition metal surfaces , 1998 .

[35]  Dale F. Rudd,et al.  The Microkinetics of heterogeneous catalysis , 1993 .

[36]  In situ ATR-IR spectroscopic and reaction kinetics studies of water-gas shift and methanol reforming on Pt/Al2O3 catalysts in vapor and liquid phases. , 2005, The journal of physical chemistry. B.

[37]  U. Graham,et al.  Low temperature water-gas shift: kinetic isotope effect observed for decomposition of surface formates for Pt/ceria catalysts , 2004 .

[38]  Polycarpos Falaras,et al.  Low-temperature water-gas shift reaction over Au/CeO2 catalysts , 2002 .

[39]  Alexandre Goguet,et al.  Spectrokinetic Investigation of Reverse Water-Gas-Shift Reaction Intermediates over a Pt/CeO2 Catalyst , 2004 .

[40]  D. Ollis,et al.  The chemistry and catalysis of the water gas shift reaction: 1. The kinetics over supported metal catalysts , 1981 .

[41]  Robert J. Farrauto,et al.  Deactivation of Pt/CeO2 water-gas shift catalysts due to shutdown/startup modes for fuel cell applications , 2005 .

[42]  Maria Flytzani-Stephanopoulos,et al.  Low-temperature water-gas shift reaction over Cu- and Ni-loaded cerium oxide catalysts , 2000 .

[43]  P. Panagiotopoulou,et al.  Effect of morphological characteristics of TiO2-supported noble metal catalysts on their activity for the water–gas shift reaction , 2004 .

[44]  D. Vlachos,et al.  A C1 mechanism for methane oxidation on platinum , 2003 .

[45]  W. Epling,et al.  Overview of the Fundamental Reactions and Degradation Mechanisms of NOx Storage/Reduction Catalysts , 2004 .

[46]  Dionisios G. Vlachos,et al.  Is the water–gas shift reaction on Pt simple?: Computer-aided microkinetic model reduction, lumped rate expression, and rate-determining step , 2005 .

[47]  G. Germani,et al.  Platinum/ceria/alumina catalysts on microstructures for carbon monoxide conversion , 2005 .

[48]  Karl Jacobi,et al.  Vibrational and structural properties of OH adsorbed on Pt(111) , 1999 .