An in-depth evaluation of surface characteristics and key machining responses in WEDM of aerospace alloy under varying electric discharge environments

[1]  S. Pervaiz,et al.  Exploring the feasibility of novel coated wires in wire EDM of Ti-6Al-4 V aerospace alloy: a case of multi-pass strategy , 2021, Journal of the Brazilian Society of Mechanical Sciences and Engineering.

[2]  Rachel E. Dianiska,et al.  A Process Perspective , 2021 .

[3]  M. Wiśniewska,et al.  Comparative analysis of WEDM with different wire electrodes applied to cut titanium Ti6Al4V , 2020 .

[4]  E. Papazoglou,et al.  Surface Topography of Ti 6Al 4V ELI after High Power EDM , 2020 .

[5]  M. Jahan,et al.  A Study on the Surface Composition and Migration of Materials and Their Effect on Surface Microhardness during Micro-EDM of Ti-6Al-4V , 2019, Journal of Materials Engineering and Performance.

[6]  A. Pramanik,et al.  Understanding the wire electrical discharge machining of Ti6Al4V alloy , 2019, Heliyon.

[7]  S. Datta,et al.  Study of surface integrity and machining performance during main/rough cut and trim/finish cut mode of WEDM on Ti–6Al–4V: effects of wire material , 2019, Journal of the Brazilian Society of Mechanical Sciences and Engineering.

[8]  S. Datta,et al.  WEDM Performance of Ti-6Al-4V: Emphasis on Multi-Cut Strategy, Effects of Electrode Wire , 2019, Materials Today: Proceedings.

[9]  S. R. Dhale Wire electrode diameter effect on cutting speed, in WEDM of varying height Inconel-718 , 2018, International Journal of Emerging Trends in Science and Technology.

[10]  Rahul,et al.  Effects of Tool Electrode on EDM Performance of Ti-6Al-4V , 2018, Silicon.

[11]  Xuyang Chu,et al.  Studies on the surface of high-performance alloys machined by micro-EDM , 2018 .

[12]  Y. Gong,et al.  Experimental study on surface quality and machinability of Ti-6Al-4V rotated parts fabricated by low-speed wire electrical discharge turning , 2018 .

[13]  Naveed Ahmed,et al.  Investigation of wire electric discharge machining of stainless-clad steel for optimization of cutting speed , 2018 .

[14]  J. Kovář,et al.  Analysis of surface and subsurface layers after WEDM for Ti-6Al-4V with heat treatment , 2018 .

[15]  Rahul,et al.  Surface Integrity and Metallurgical Characteristics of the EDMed Work Surfaces of A2 Tool Steel (SAE 304SS), Inconel 601 and Ti-6Al-4V: a Comparative Analysis , 2018, Silicon.

[16]  Tjprc,et al.  Effect of Process Parameters on the Surface Integrity of Micro-Holes of TI6AL4V Obtained by Micro-EDM , 2018 .

[17]  Diego Carou,et al.  Experimental study for the effective and sustainable repair and maintenance of bars made of Ti-6Al-4V alloy. Application to the aeronautic industry , 2017 .

[18]  Md. Zurais Ibne Ashraf,et al.  Crystallinity, surface morphology, and chemical composition of the recast layer and rutile-TiO2 formation on Ti-6Al-4V ELI by wire-EDM to enhance biocompatibility , 2017 .

[19]  Y. Gong,et al.  Modeling and experimental study on breakdown voltage (BV) in low speed wire electrical discharge machining (LS-WEDM) of Ti-6Al-4V , 2017 .

[20]  M. Jahan,et al.  A Comparative Study on Micro-electro-discharge-machined Surface Characteristics of Ni-Ti and Ti-6Al-4V with Respect to Biocompatibility , 2017 .

[21]  Siva Prasad Arikatla,et al.  Surface Integrity Characteristics in Wire Electrical Discharge Machining of Titanium Alloy during Main cut and Trim cuts , 2017 .

[22]  Priyaranjan Sharma,et al.  Effect of wire diameter on surface integrity of wire electrical discharge machined Inconel 706 for gas turbine application , 2016 .

[23]  Amit Rai Dixit,et al.  Modeling and Optimization of Machining Nimonic C-263 Superalloy using Multicut Strategy in WEDM , 2016 .

[24]  Ch. V. S. ParameswaraRao,et al.  Studies on Wire Selection for Machining With W E D M , 2016 .

[25]  V. Kumar,et al.  An experimental study on trim cutting operation using metal powder mixed dielectric in WEDM of Nimonic-90 , 2016 .

[26]  Ahmed A. D. Sarhan,et al.  Review of improvements in wire electrode properties for longer working time and utilization in wire EDM machining , 2015 .

[27]  Lida Shen,et al.  Study of multi-cutting by WEDM for specific crystallographic planes of monocrystalline silicon , 2015 .

[28]  Kamal Kumar Jangra,et al.  An experimental study for multi-pass cutting operation in wire electrical discharge machining of WC-5.3% Co composite , 2015 .

[29]  V. Krishnaraj,et al.  Effect of multipass cutting on surface roughness in wire electrical discharge machining of metal matrix composites , 2014 .

[30]  J. F. Liu,et al.  Surface integrity evolution from main cut mode to finish trim cut mode in W-EDM of shape memory alloy , 2014 .

[31]  S. I. Jaffery,et al.  Effect of Current in the EDM Machining of Aluminum 6061 T6 and its Effect on the Surface Morphology , 2014 .

[32]  Xianglin Zhang,et al.  Surface Integrity of Tool Steels Multi-cut by Wire Electrical Discharge Machining☆ , 2014 .

[33]  Yuebin B. Guo,et al.  Surface Integrity Characteristics in Wire-EDM of Inconel 718 at Different Discharge Energy , 2013 .

[34]  J. Davim,et al.  REVIEW ON MACHINABILITY OF TITANIUM ALLOYS: THE PROCESS PERSPECTIVE , 2013 .

[35]  Kamlakar P Rajurkar,et al.  Electrical discharge machining of Ti6Al4V with a bundled electrode , 2012 .

[36]  Fritz Klocke,et al.  Surface integrity evolution of powder metallurgical tool steel by main cut and finishing trim cuts in wire-EDM , 2011 .

[37]  Bijoy Bhattacharyya,et al.  An Integrated Approach to Optimization of WEDM Combining Single-Pass and Multipass Cutting Operation , 2010 .

[38]  David K. Aspinwall,et al.  Workpiece surface roughness and integrity after WEDM of Ti–6Al–4V and Inconel 718 using minimum damage generator technology , 2008 .

[39]  U. Çaydas,et al.  Electrical discharge machining of titanium alloy (Ti–6Al–4V) , 2007 .

[40]  Ulaş Çaydaş,et al.  A comparative study of surface integrity of Ti–6Al–4V alloy machined by EDM and AECG , 2007 .

[41]  M. S. Shunmugam,et al.  Characteristics of wire-electro discharge machined Ti6Al4V surface , 2004 .

[42]  L. Munuera,et al.  In vitro corrosion behaviour and osteoblast response of thermally oxidised Ti6Al4V alloy. , 2003, Biomaterials.

[43]  Shane Y. Hong,et al.  New cooling approach and tool life improvement in cryogenic machining of titanium alloy Ti-6Al-4V , 2001 .

[44]  G. Byrne,et al.  Observations on chip formation and acoustic emission in machining Ti–6Al–4V alloy , 2001 .

[45]  C. Richard Liu,et al.  MACHINING TITANIUM AND ITS ALLOYS , 1999 .