Caracterização textural, morfológica e estrutural de catalisadores automotivos novos e usados

Catalytic converters or automotive catalyst are formed by noble metals such as platinum, rhodium, palladium, and molybdenum supported in cordierite, a porous ceramic materials which convert the pollutant gases in carbon dioxide, water and nitrogenous, no-pollutant products. In this work, we discuss the deactivation of automotive catalyst due to the high operation temperature and by inorganic contaminants originating in engine oil and fuel. New and used catalysts were analyzed by gas adsorption, picnometry, X-ray diffraction, thermal analyses and scanning electron microscopy for textural, morphological and structural characterization. EDS and WDS electron microprobe were used to detect the composition of the catalysts and their contaminants.

[1]  Grigorios C. Koltsakis,et al.  CATALYTIC AUTOMOTIVE EXHAUST AFTERTREATMENT , 1997 .

[2]  M. C. R. Rangel,et al.  Impacto dos catalisadores automotivos no controle da qualidade do ar , 2003 .

[3]  T. Horiuchi,et al.  Improvement of thermal stability of alumina by addition of zirconia , 1999 .

[4]  A. Trovarelli,et al.  Remarkable stabilization of transition alumina operated by ceria under reducing and redox conditions , 2000 .

[5]  G. Sandoval,et al.  Surface and catalytic properties of Al2O3–ZrO2 solid solutions prepared by sol–gel methods , 2000 .

[6]  J. T. Kummer,et al.  Catalysts for automobile emission control , 1980 .

[7]  J. Kašpar,et al.  Stabilisation of nanostructured Ce0.2Zr0.8O2 solid solution by impregnation on Al2O3: a suitable method for the production of thermally stable oxygen storage/release promoters for three-way catalysts , 2000 .

[8]  C. Larese Deactivation of real three way catalysts by CePO4 formation , 2003 .

[9]  F. B. Noronha,et al.  The role of Ni on the performance of automotive catalysts: evaluating the ethanol oxidation reaction , 2003 .

[10]  G. Magnacca,et al.  Surface characterization of modified aluminas. Part 4.—Surface hydration and Lewis acidity of CeO2–Al2O3 systems , 1996 .

[11]  M. Pijolat,et al.  Influence of surface area and additives on the thermal stability of transition alumina catalyst supports. II: Kinetic model and interpretation , 1987 .

[12]  D. D. Beck,et al.  Axial characterization of oxygen storage capacity in close-coupled lightoff and underfloor catalytic converters and impact of sulfur , 1997 .

[13]  J. Vohs,et al.  An Examination of Sulfur Poisoning on Pd/Ceria Catalysts , 2002 .

[14]  D. D. Beck,et al.  Impact of sulfur on the performance of vehicle-aged palladium monoliths , 1995 .

[15]  F. Oudet,et al.  Thermal stabilization of transition alumina by structural coherence with LnAlO3 (Ln = La, Pr, Nd) , 1988 .

[16]  J. Z. Shyu,et al.  Surface characterization of alumina-supported ceria , 1988 .

[17]  G. Koltsakis,et al.  Effect of perturbations in the exhaust gas composition on three-way catalyst light off , 2003 .

[18]  J. Z. Shyu,et al.  Characterization of Pd/γ-alumina catalysts containing ceria , 1988 .

[19]  M. Shelef,et al.  Effects of sulphur on noble metal automotive catalysts , 1991 .