Энергосберегающая технология сорбитизации высокоуглеродистой катанки в потоке стана 150 ОАО «БМЗ – управляющая компания холдинга «БМК»
暂无分享,去创建一个
Peculiarities of structure formation of steel 80K after austenization with the subsequent cooling with speed ~15 °С/sec within 1-20 seconds and with final cooling in water are studied. The scientifically reasonable energy saving models of a sorbitizing of high-carbon wire rood, which allow to lower energy consumption while maintaining the pace of productions and provision o of the necessary quality and process performance are developed and implemented on the mill 150 OJSC «BSW – MHC «BMC».