Effect of MoSi2 Particles on the Fracture Toughness of AlN-, SiC-, and Si3N4-based Ceramics

The effect of 30 vol% MoSi2 addition on the fracture toughness of AlN-, SiC-, and Si3N4-based composites is investigated. To isolate the contribution of MoSi2 particulate, the toughness of the composite is compared to that of the reference AlN, SiC, and Si 3N4 matrixes. It turns out that the main toughening mechanisms are residual stress and crack deflection. The residual stress is evaluated through the strain measure in the reinforcing particles by X-ray diffraction, and the crack deflection by analysis of the crack paths. The overall toughening effect is calculated as the sum of these two contributions compared to the experimental values of the toughness of the composites.

[1]  A. Evans,et al.  Crack‐Growth Resistance of Microcracking Brittle Materials , 2006 .

[2]  D. Sciti,et al.  Analysis of residual stresses in ternary electroconductive composites , 2006 .

[3]  D. Butt,et al.  Mechanical Behavior of MoSi2 Reinforced–Si3N4Matrix Composites , 2005 .

[4]  D. Sciti,et al.  Microstructure and mechanical properties of novel ternary electroconductive ceramics , 2004 .

[5]  D. Sciti,et al.  High-Temperature Resistant Composites in the AlN—SiC—MoSi2 System. , 2004 .

[6]  D. Sciti,et al.  Effects of additives on densification, microstructure and properties of liquid-phase sintered silicon carbide , 2000 .

[7]  Wei Yang,et al.  Toughening mechanisms of nano-composite ceramics , 1998 .

[8]  J. Petrovic,et al.  Fracture Modes in MoSi2 , 1992 .

[9]  T. Hirano,et al.  Elastic constants of MoSi2 and WSi2 single crystals , 1990 .

[10]  R. Winholtz,et al.  Residual Stresses in a Wo‐Phase Microcracking Ceramic , 1990 .

[11]  F.,et al.  Microstructural Design Of Toughened Ceramics , 1990 .

[12]  M. Taya,et al.  Toughening of a particulate-reinforced/ceramic-matrix composite. Technical report , 1989 .

[13]  R. Bradt,et al.  Thermoelastic Micromechanical Stresses Associated with a Large α‐Silicon Carbide Grain in a Polycrystalline β‐Silicon Carbide Matrix , 1989 .

[14]  Anthony G. Evans,et al.  Crack deflection processes—I. Theory , 1983 .

[15]  D. Munz,et al.  Fracture toughness calculation from maximum load in four point bend tests of chevron notch specimens , 1980 .

[16]  F. F. Lange,et al.  The interaction of a crack front with a second-phase dispersion , 1970 .