Effect of clad orientation on the mechanical properties of laser-clad repaired ultra-high strength 300 M steel
暂无分享,去创建一个
S. Palanisamy | M. Dargusch | R. Rashid | C. Barr | N. Orchowski | N. Matthews | K. Nazari
[1] S. Palanisamy,et al. Effect of laser reheat post-treatment on the microstructural characteristics of laser-cladded ultra-high strength steel , 2019, Surface and Coatings Technology.
[2] Jianjun Li,et al. In-situ investigation of phase transformation behaviors of 300M steel in continuous cooling process , 2018, Materials Characterization.
[3] Guang Yang,et al. Microstructure and tensile properties of laser engineered net shaped reduced activation ferritic/martensitic steel , 2018, Materials Characterization.
[4] Eduard Hryha,et al. Effect of build geometry on the microstructural development of 316L parts produced by additive manufacturing , 2018, Materials Characterization.
[5] S. Palanisamy,et al. Effect of energy per layer on the anisotropy of selective laser melted AlSi12 aluminium alloy , 2018, Additive Manufacturing.
[6] M. Easton,et al. Influence of macrosegregation on solidification cracking in laser clad ultra-high strength steels , 2018 .
[7] Shu Beng Tor,et al. Anisotropy and heterogeneity of microstructure and mechanical properties in metal additive manufacturing: A critical review , 2018 .
[8] Lonnie J. Love,et al. On the toughness scatter in low alloy C-Mn steel samples fabricated using wire arc additive manufacturing , 2018 .
[9] M. Easton,et al. In-situ quench and tempering for microstructure control and enhanced mechanical properties of laser cladded AISI 420 stainless steel powder on 300M steel substrates , 2018 .
[10] Syed H. Masood,et al. Effect of scan strategy on density and metallurgical properties of 17-4PH parts printed by Selective Laser Melting (SLM) , 2017 .
[11] S. Palanisamy,et al. Metallurgical and geometrical characterisation of the 316L stainless steel clad deposited on a mild steel substrate , 2017 .
[12] U. Ramamurty,et al. Mechanical behavior of selective laser melted 316L stainless steel , 2017 .
[13] Zemin Wang,et al. Comparison on mechanical anisotropies of selective laser melted Ti-6Al-4V alloy and 304 stainless steel , 2017 .
[14] A. Elwany,et al. Mechanical properties and microstructural characterization of selective laser melted 17-4 PH stainless steel , 2017 .
[15] Peng Guo,et al. Study on microstructure, mechanical properties and machinability of efficiently additive manufactured AISI 316L stainless steel by high-power direct laser deposition , 2017 .
[16] Bo Cheng,et al. Stress and deformation evaluations of scanning strategy effect in selective laser melting , 2016 .
[17] Hua-ming Wang,et al. Microstructure characterization and mechanical behavior of laser additive manufactured ultrahigh-strength AerMet100 steel , 2016 .
[18] Chun H. Wang,et al. Fatigue and fracture behavior of laser clad repair of AerMet® 100 ultra-high strength steel , 2016 .
[19] T. Mower,et al. Mechanical behavior of additive manufactured, powder-bed laser-fused materials , 2016 .
[20] K. Dawson,et al. Mechanical response and deformation mechanisms of ferritic oxide dispersion strengthened steel structures produced by selective laser melting , 2015 .
[21] I. Manna,et al. Microstructure and Mechanical Properties of Laser Clad and Post-cladding Tempered AISI H13 Tool Steel , 2015, Metallurgical and Materials Transactions A.
[22] Rui Vilar,et al. Repair and manufacturing of single crystal Ni-based superalloys components by laser powder deposition—A review , 2015 .
[23] Thomas Niendorf,et al. Microstructural Characterization and Mechanical Performance of Hot Work Tool Steel Processed by Selective Laser Melting , 2015, Metallurgical and Materials Transactions B.
[24] C. Tuck,et al. Effect of the build orientation on the mechanical properties and fracture modes of SLM Ti–6Al–4V , 2014 .
[25] Vladimir Luzin,et al. Effect of laser clad repair on the fatigue behaviour of ultra-high strength AISI 4340 steel , 2014 .
[26] Jacqueline Lecomte-Beckers,et al. Microstructures and Mechanical Properties of Stainless Steel AISI 316L Processed by Selective Laser Melting , 2014 .
[27] Thomas Tröster,et al. On the fatigue crack growth behavior in 316L stainless steel manufactured by selective laser melting , 2014 .
[28] S. Aihara,et al. A simulation model for cleavage crack propagation in bcc polycrystalline solids , 2011 .
[29] Weidong Huang,et al. Influence of laser deposition patterns on part distortion, interior quality and mechanical properties by laser solid forming (LSF) , 2011 .
[30] A. Esnaola,et al. Study of mechanical properties of AISI 316 stainless steel processed by “selective laser melting”, following different manufacturing strategies , 2010 .
[31] S. Lynch,et al. A brief history of fractography , 2006 .
[32] A. M. Deus,et al. Rapid tooling by laser powder deposition : Process simulation using finite element analysis , 2005 .
[33] Gerry Byrne,et al. Laser cladding of aerospace materials , 2002 .
[34] F. Prinz,et al. Thermal stresses and deposition patterns in layered manufacturing , 2001 .
[35] N. Matthews,et al. Additive Metal Technologies for Aerospace Sustainment , 2018 .
[36] Chun H. Wang,et al. Quantitative fractography and modelling of fatigue crack propagation in high strength AerMet®100 steel repaired with a laser cladding process , 2017 .
[37] Alaa Elwany,et al. Effects of building orientation and heat treatment on fatigue behavior of selective laser melted 17-4 PH stainless steel , 2017 .
[38] S. Aihara,et al. Simulation of Cleavage Crack Propagation in Steels with Anisotropic Crystal Orientation Distribution , 2014 .
[39] J. Knott,et al. Charpy-impact-toughness prediction using an “effective” grain size for thermomechanically controlled rolled microalloyed steels , 2004 .
[40] Frank W. Liou,et al. Laser Aided Part Repair-a Review , 2002 .