The evaluation of nickel deposit obtained via Watts electrolyte at ambient temperature

[1]  A. A. Mohamad,et al.  The production of nickel–alumina composite coating via electroplating , 2009 .

[2]  H. Tian,et al.  Effects of peak current density on the mechanical properties of nanocrystalline Ni-Co alloys produced by pulse electrodeposition , 2008 .

[3]  T. Matencio,et al.  Effect of the Current Density on Morphology, Porosity, and Tribological Properties of Electrodeposited Nickel on Copper , 2008, Journal of Materials Engineering and Performance.

[4]  Zhixing Wang,et al.  Nickel electrodeposition from novel citrate bath , 2007 .

[5]  J. Celis,et al.  Tribocorrosion behaviour of Ni–SiC nano-structured composite coatings obtained by electrodeposition , 2007 .

[6]  A. Lasia,et al.  Study of the hydrogen evolution reaction on nickel-based composite coatings containing molybdenum powder , 2007 .

[7]  Tingju Li,et al.  Preparation of nanostructured Ni/Al2O3 composite coatings in high magnetic field , 2007 .

[8]  S. Aruna,et al.  Synthesis and properties of electrodeposited Ni/ceria nanocomposite coatings , 2006 .

[9]  K. Ibrahim,et al.  Enhancement of wear resistance of ductile cast iron by Ni–SiC composite coating , 2006 .

[10]  C. Gheorghieș,et al.  Preparation and structural characterization of nickel/ alumina nano-particles composite coatings , 2006 .

[11]  V. N. Misra,et al.  Effect of thiourea during nickel electrodeposition from acidic sulfate solutions , 2005 .

[12]  Shiyun Dong,et al.  Electrodepositing nickel silica nano-composites coatings , 2005 .

[13]  V. Ganesh,et al.  Fine grain growth of nickel electrodeposit: effect of applied magnetic field during deposition , 2005 .

[14]  M. Ger Electrochemical deposition of nickel/SiC composites in the presence of surfactants , 2004 .

[15]  M. Monev,et al.  Hydrogen coevolution and permeation in nickel electroplating , 2003 .

[16]  K. I. Popov,et al.  Fundamental Aspects of Electrometallurgy , 2002 .

[17]  G. DiBari Chronology of nickel electroplating , 2002 .

[18]  N. Mandich,et al.  Understanding and troubleshooting decorative nickel electroplating systems-part I: Introduction and brightness problems , 2002 .

[19]  B. Beverskog,et al.  Revised Pourbaix diagrams for nickel at 25-300°C , 1997 .

[20]  M. Pourbaix Atlas of Electrochemical Equilibria in Aqueous Solutions , 1974 .

[21]  S. Beloglazov Absorption of hydrogen by steel during pickling and electroplating , 1966 .