Measurement of liquid water content in cathode gas diffusion electrode of polymer electrolyte fuel cell

Water management in cathode gas diffusion electrode (GDE) of polymer electrolyte fuel cell (PEFC) is essential for high performance operation, because liquid water condensed in porous gas diffusion layer (GDL) and catalyst layer (CL) blocks oxygen transport to active reaction sites. In this study, the average liquid water content inside the cathode GDE of a low-temperature PEFC is experimentally and quantitatively estimated by the weight measurement, and the relationship between the water accumulation rate in the cathode GDE and the cell voltage is investigated. The liquid water behavior at the cathode is also visualized using an optical diagnostic, and the effects of operating conditions and GDL structures on the water transport in the cathode GDE are discussed. It is found that the liquid water content in the cathode GDE increases remarkably after starting the fuel cell operation due to the water production at the CL. At a high current density, the cell voltage drops suddenly after starting the operation in spite of a low water content in the cathode GDE. When the GDL thickness is increased, much water accumulates near the cathode CL and the fuel cell shuts down immediately after the operation. In the final section of this paper, the structure of cathode GDL that has several grooves for water removal is proposed to prevent water flooding and improve fuel cell performance. This groove structure is effective to promote the removal of the liquid water accumulated near the active catalyst sites.

[1]  Alan K. Thompson,et al.  Neutron Imaging Technique for In Situ Measurement of Water Transport Gradients within Nafion in Polymer Electrolyte Fuel Cells , 1999 .

[2]  C. Hebling,et al.  Visualization of water buildup in the cathode of a transparent PEM fuel cell , 2003 .

[3]  Alexander Wokaun,et al.  In situ observation of the water distribution across a PEFC using high resolution neutron radiography , 2008 .

[4]  Christoph Ziegler,et al.  Enhancing liquid water transport by laser perforation of a GDL in a PEM fuel cell , 2008 .

[5]  M. Fowler,et al.  In-plane and through-plane gas permeability of carbon fiber electrode backing layers , 2006 .

[6]  Marc Prat,et al.  Scale effect and two-phase flow in a thin hydrophobic porous layer. Application to water transport in gas diffusion layers of proton exchange membrane fuel cells , 2009 .

[7]  David L. Jacobson,et al.  In situ neutron imaging technique for evaluation of water management systems in operating PEM fuel cells , 2004 .

[8]  Mark Pritzker,et al.  Pore network modeling of fibrous gas diffusion layers for polymer electrolyte membrane fuel cells , 2007 .

[9]  T. Nguyen,et al.  Two-phase flow model of the cathode of PEM fuel cells using interdigitated flow fields , 2000 .

[10]  Shohji Tsushima,et al.  Microscopic Visualization of State and Behavior of Liquid Water in a Gas Diffusion Layer of PEFC , 2007 .

[11]  T. Springer,et al.  Polymer Electrolyte Fuel Cell Model , 1991 .

[12]  Chao-Yang Wang,et al.  Liquid water transport in a mixed-wet gas diffusion layer of a polymer electrolyte fuel cell , 2008 .

[13]  Jack S. Brenizer,et al.  Quantification of liquid water accumulation and distribution in a polymer electrolyte fuel cell using neutron imaging , 2006 .

[14]  N. Djilali,et al.  Ex situ visualization of liquid water transport in PEM fuel cell gas diffusion layers , 2006 .

[15]  Chang-Soo Kim,et al.  X-ray imaging of water distribution in a polymer electrolyte fuel cell , 2008 .

[16]  Z. H. Wang,et al.  Two-phase flow and transport in the air cathode of proton exchange membrane fuel cells , 2000 .

[17]  D. Wilkinson,et al.  Aging mechanisms and lifetime of PEFC and DMFC , 2004 .