Ion nitriding of a superaustenitic stainless steel: Wear and corrosion characterization

[1]  S. Nagarajan,et al.  Crevice corrosion behaviour of superaustenitic stainless steels: Dynamic electrochemical impedance spectroscopy and atomic force microscopy studies , 2009 .

[2]  J. Fisher,et al.  The damage tolerance of S-phase coated biomedical grade stainless steel , 2007 .

[3]  A. P. Tschiptschin,et al.  On the formation of expanded austenite during plasma nitriding of an AISI 316L austenitic stainless steel , 2006 .

[4]  J. Baranowska,et al.  Corrosion resistance of nitrided layers on austenitic steel , 2006 .

[5]  P. Ferro,et al.  Microstructural, compositional and residual stress evaluation of CO2 laser welded superaustenitic AISI 904L stainless steel , 2006 .

[6]  S. E. Franklin,et al.  Tribological behaviour and mechanical properties of low temperature gas nitrided austenitic steel in relation to layer morphology , 2005 .

[7]  X. Zhu,et al.  Plasma-based low-energy ion implantation of austenitic stainless steel for improvement in wear and corrosion resistance , 2005 .

[8]  B. Karlsson,et al.  Cyclic deformation and fatigue behaviour of 7Mo–0.5N superaustenitic stainless steel—stress–strain relations and fatigue life , 2001 .

[9]  K. Rie,et al.  Improvement of the mechanical properties of austenitic stainless steel after plasma nitriding , 2000 .

[10]  S. Heino Role of Mo and W during sensitization of superaustenitic stainless steel—crystallography and composition of precipitates , 2000 .

[11]  J. Bringas,et al.  Practical handbook of stainless steels & nickel alloys , 1999 .

[12]  T. Bell,et al.  Sliding wear characteristics of low temperature plasma nitrided 316 austenitic stainless steel , 1998 .