About the role of iron on the alteration of simplified nuclear glasses in deaerated solutions at 50°C

[1]  N. Hyatt,et al.  Corrosion of the International Simple Glass under acidic to hyperalkaline conditions , 2018, npj Materials Degradation.

[2]  D. Strachan Glass dissolution as a function of pH and its implications for understanding mechanisms and future experiments , 2017 .

[3]  P. Frugier,et al.  Impact of iron and magnesium on glass alteration: Characterization of the secondary phases and determination of their solubility constants , 2017 .

[4]  Marie Collin,et al.  Atom-Probe Tomography, TEM and ToF-SIMS study of borosilicate glass alteration rim: A multiscale approach to investigating rate-limiting mechanisms , 2017 .

[5]  P. Frugier,et al.  Mineralogy and thermodynamic properties of magnesium phyllosilicates formed during the alteration of a simplified nuclear glass , 2016 .

[6]  S. Gin,et al.  Effect of natural and synthetic iron corrosion products on silicate glass alteration processes , 2016 .

[7]  P. Frugier,et al.  Reactive transport processes occurring during nuclear glass alteration in presence of magnetite , 2015 .

[8]  P. Frugier,et al.  Origin and consequences of silicate glass passivation by surface layers , 2015, Nature Communications.

[9]  S. Gin,et al.  The fate of silicon during glass corrosion under alkaline conditions: A mechanistic and kinetic study with the International Simple Glass , 2015 .

[10]  M. Schlegel,et al.  Corrosion of metal iron in contact with anoxic clay at 90 °C: Characterization of the corrosion products after two years of interaction , 2014 .

[11]  M. Tabarant,et al.  Hydrogen absorption associated with the corrosion mechanism of 316L stainless steels in primary medium of Pressurized Water Reactor (PWR) , 2014 .

[12]  P. Frugier,et al.  New Insight into the Residual Rate of Borosilicate Glasses: Effect of S/V and Glass Composition , 2013 .

[13]  S. Gin,et al.  Effect of iron metal and siderite on the durability of simulated archeological glassy material , 2013 .

[14]  Eric M. Pierce,et al.  Monte Carlo Simulations of the Corrosion of Aluminoborosilicate Glasses , 2013 .

[15]  S. Gin,et al.  Impact of iron on nuclear glass alteration in geological repository conditions: A multiscale approach , 2013 .

[16]  S. Gin,et al.  Silicate glass alteration enhanced by iron: origin and long-term implications. , 2013, Environmental science & technology.

[17]  P. Frugier,et al.  SON68 Glass Alteration Enhanced by Magnetite , 2013 .

[18]  K. Emmerich Full Characterization of Smectites , 2013 .

[19]  S. Gin,et al.  Effect of composition on the short-term and long-term dissolution rates of ten borosilicate glasses of increasing complexity from 3 to 30 oxides , 2012 .

[20]  P. Frugier,et al.  Characterization of Alteration Phases on HLW Glasses After 15 Years of PCT Leaching , 2012 .

[21]  Christophe Poinssot,et al.  Long-term Behavior Science: The cornerstone approach for reliably assessing the long-term performance of nuclear waste , 2012 .

[22]  P. Frugier,et al.  Glass–water interphase reactivity with calcium rich solutions , 2011 .

[23]  F. Jomard,et al.  Mechanism of hydrogen absorption during the exposure of alloy 600-like single-crystals to PWR primary simulated media , 2011 .

[24]  S. Gin,et al.  Glass–iron–clay interactions in a radioactive waste geological disposal: An integrated laboratory-scale experiment , 2011 .

[25]  P. Frugier,et al.  Composition effects on synthetic glass alteration mechanisms: Part 1. Experiments , 2010 .

[26]  G. Calas,et al.  Structural evolution of glass surface during alteration: Application to nuclear waste glasses , 2010 .

[27]  S. Gin,et al.  Structural identification of a trioctahedral smectite formed by the aqueous alteration of a nuclear glass , 2010 .

[28]  M. Schlegel,et al.  Anodic activation of iron corrosion in clay media under water-saturated conditions at 90 degrees C: characterization of the corrosion interface. , 2010, Environmental science & technology.

[29]  Patrick Jollivet,et al.  Insight into silicate-glass corrosion mechanisms. , 2008, Nature materials.

[30]  Michel Soustelle,et al.  Experimental tests to validate the rate-limiting step assumption used in the kinetic analysis of solid-state reactions , 2008 .

[31]  Jean-Eric Lartigue,et al.  SON68 nuclear glass dissolution kinetics: Current state of knowledge and basis of the new GRAAL model , 2008 .

[32]  M. Schlegel,et al.  Metal corrosion and argillite transformation at the water-saturated, high-temperature iron–clay interface: A microscopic-scale study , 2008 .

[33]  R. J. Hand,et al.  Property modification of a high level nuclear waste borosilicate glass through the addition of Fe2O3 , 2008 .

[34]  Amanda G. Turner,et al.  Intracrystalline boron isotope partitioning in illite-smectite: Testing the geothermometer , 2007 .

[35]  S. Gin,et al.  Hydrogen–sodium interdiffusion in borosilicate glasses investigated from first principles , 2006 .

[36]  Andrei V. Bandura,et al.  The Ionization Constant of Water over Wide Ranges of Temperature and Density , 2006 .

[37]  M. Shibata,et al.  The effect of iron on montmorillonite stability. (II) Experimental investigation , 2006 .

[38]  P. Barboux,et al.  The role of aluminium in the durability of alumino- borosilicate glasses , 2005 .

[39]  S. Gin,et al.  17O 3Q-MAS NMR characterization of a sodium aluminoborosilicate glass and its alteration gel , 2001 .

[40]  I. Hutcheon,et al.  Boron isotope geochemistry during diagenesis. Part I. Experimental determination of fractionation during illitization of smectite , 2001 .

[41]  S. Gin,et al.  SON 68 nuclear glass alteration kinetics between pH 7 and pH 11.5 , 2001 .

[42]  S. Gin,et al.  Alteration kinetics of a simplified nuclear glass in an aqueous medium: effects of solution chemistry and of protective gel properties on diminishing the alteration rate , 2000 .

[43]  S. Kim,et al.  Effects of Metals, Metal Oxides and Metal Hydroxide on the Leaching of Simulated Nuclear Waste Glass , 1997 .

[44]  H. Furuya,et al.  Effects of Redox Condition on Waste Glass Corrosion in the Presence of Magnetite , 1995 .

[45]  B. C. Bunker,et al.  Molecular mechanisms for corrosion of silica and silicate glasses , 1994 .

[46]  J. Edmond,et al.  The sedimentary cycle of the boron isotopes , 1987 .

[47]  H. Zwicky,et al.  Borosilicate Glass Corrosion in the Presence of Steel Corrosion Products , 1986 .

[48]  N. Binsted,et al.  Fe K-EDGE X-RAY ABSORPTION SPECTROSCOPY OF SILICATE MINERALS AND GLASSES , 1986 .

[49]  J. Charbonnier,et al.  Quantitative surface analysis by glow discharge optical spectrometry , 1986 .

[50]  B. Grambow,et al.  Modeling of the Effect of Iron Corrosion Products on Nuclear Waste Glass Performance , 1986 .

[51]  J. Pons-Corbeau Study of emission and sputtering yields in some alloys and oxide by glow discharge optical spectrometry: Quantification of analysis , 1985 .

[52]  K. Fox,et al.  Transition metal ions in silicate melts. Part 2. Iron in sodium silicate glasses , 1982 .

[53]  B. A. Fleming,et al.  Silicic acid ionization and calculation of silica solubility at elevated temperature and pH application to geothermal fluid processing and reinjection , 1982 .