Environmentally Enhanced Fracture of Glass: A Historical Perspective
暂无分享,去创建一个
Stephen W. Freiman | John J. Mecholsky | Sheldon M. Wiederhorn | J. J. Mecholsky | S. Wiederhorn | S. Freiman
[1] Hiroyuki Abe,et al. Subcritical Crack Growth in Silica Optical Fibers in Wide Range of Crack Velocities , 1996 .
[2] C. Ullner,et al. Fatigue limit and crack arrest in alkali-containing silicate glasses , 1991 .
[3] J. Murgatroyd. Mechanism of Brittle Rupture , 1944, Nature.
[4] H. Johnson,et al. Fracture of Glass in Vacuum , 1974 .
[5] Y. Hibino,et al. Crack Growth in Silica Glass Under Dynamic Loading , 2006 .
[6] J. Guin,et al. Surfaces formed by subcritical crack growth in silicate glasses , 2006 .
[7] J. Gilman,et al. Direct Measurements of the Surface Energies of Crystals , 1960 .
[8] F W Preston,et al. The structure of abraded glass surfaces , 1922 .
[9] The Effect of the Surrounding Atmosphere on the Delayed Fracture of Glass , 1949 .
[10] E. Orowan. The Fatigue of Glass Under Stress , 1944, Nature.
[11] P. Gibbs,et al. On the Fracture of Glass Which Is Subjected to Slowly Increasing Stress , 1951 .
[12] T. Baker,et al. Fatigue of Glass under Static Loads , 1946 .
[13] C. Inglis. Stresses in a plate due to the presence of cracks and sharp corners , 1913 .
[14] D. M. Marsh. Plastic flow and fracture of glass , 1964, Proceedings of the Royal Society of London. Series A. Mathematical and Physical Sciences.
[15] R. Dauskardt,et al. Fracture of nanoporous methyl silsesquioxane thin-film glasses , 2006 .
[16] Irving Langmuir. THE CONSTITUTION AND FUNDAMENTAL PROPERTIES OF SOLIDS AND LIQUIDS. PART I. SOLIDS. , 1916 .
[17] A. A. Griffith. The Phenomena of Rupture and Flow in Solids , 1921 .
[18] Sheldon M. Wiederhorn,et al. Fracture Surface Energy of Glass , 1969 .
[19] B. Lawn. Physics of Fracture , 1983 .
[20] R. Dauskardt,et al. Fracture of nanoporous thin-film glasses , 2004, Nature materials.
[21] Joseph S. Hayden,et al. Subcritical Crack Growth in a Phosphate Laser Glass , 2004 .
[22] S. Freiman. Effect of Alcohols on Crack Propagation in Glass , 1974 .
[23] Cenk Kocer,et al. Measurement of very slow crack growth in glass , 2001 .
[24] Real‐Time Observation of a Non‐Equilibrium Liquid Condensate Confined at Tensile Crack Tips in Oxide Glasses , 2005, cond-mat/0509209.
[25] S. Freiman,et al. Corrosion and Crack Growth in 33% Na2O-67% SiO2 and 33% Li2O-67% SiO2 Glasses , 1986 .
[26] Dynamic condensation of water at crack tips in fused silica glass , 2007, 0704.2531.
[27] J. L. Glathart,et al. The Effect of Temperature on the Strength and Fatigue of Glass Rods , 1946 .
[28] Crack growth threshold in soda lime silicate glass: role of hold-time , 2003 .
[29] H. Johnson,et al. Effect of Electrolyte pH on Crack Propagation in Glass , 1973 .
[30] S. Wiederhorn,et al. Estimation of ion exchange layers for soda-lime-silicate glass from curvature measurements , 2006 .
[31] L. Hench,et al. The effect of environment on silica fracture: Vacuum, carbon monoxide, water and nitrogen , 1998 .
[32] S. Freiman,et al. Effect of Corrosion Processes on Subcritical Crack Growth in Glass , 1981 .
[33] C. Janssen,et al. Specimen for fracture mechanics studies on glass , 1977 .
[34] T. Michalske. The Stress Corrosion Limit: Its Measurement and Implications , 1983 .
[35] Terry A. Michalske,et al. Steric Effects in Stress Corrosion Fracture of Glass , 1987 .
[36] The Strength of Inorganic Glasses , 1967 .
[37] Irving Langmuir,et al. The constitution and fundamental properties of solids and liquids. Part II.—Liquids , 1917 .
[38] S. Wiederhorn,et al. Crack‐Tip Structure in Soda–Lime–Silicate Glass , 2005 .
[39] J. L. Glathart,et al. The Fatigue Modulus of Glass , 1946 .
[40] F. W. Preston. The Mechanical Properties of Glass , 1942 .
[41] W. Wang,et al. Fracture of brittle metallic glasses: brittleness or plasticity. , 2005, Physical review letters.
[42] D. S. Dugdale. Yielding of steel sheets containing slits , 1960 .
[43] Stephen W. Freiman,et al. A molecular interpretation of stress corrosion in silica , 1982, Nature.
[44] B. Bunker,et al. Effect of surface stress on stress corrosion of silicate glass , 1989 .
[45] S. W. Freiman,et al. Effects of water and other dielectrics on crack growth , 1982 .
[46] S. Yalkowsky,et al. Handbook of aqueous solubility data , 2003 .
[47] A quantum chemical mechanism for the water-initiated decomposition of silica , 2003 .
[48] Edwin R. Fuller,et al. Micromechanisms of crack growth in ceramics and glasses in corrosive environments , 1980 .
[49] Sheldon M. Wiederhorn,et al. Influence of Water Vapor on Crack Propagation in Soda‐Lime Glass , 1967 .
[50] Elisabeth Bouchaud,et al. Nano-ductile crack propagation in glasses under stress corrosion: spatiotemporal evolution of damage in the vicinity of the crack tip , 2005 .
[51] S. Wiederhorn,et al. Fracture of silicate glasses: ductile or brittle? , 2004, Physical review letters.
[52] S. Wiederhorn,et al. Stress Corrosion and Static Fatigue of Glass , 1970 .
[53] E. Fuller,et al. Environmentally Enhanced Crack Growth in Soda-Lime Glass , 1985 .
[54] T. Michalske,et al. A Molecular Mechanism for Stress Corrosion in Vitreous Silica , 1983 .
[55] Anomalous temperature dependence of sub-critical crack growth in silica glass , 2003 .
[56] Dependence of Ultimate Strength of Glass Under Constant Load on Temperature, Ambient Atmosphere, and Time , 1953 .
[57] T. Michalske,et al. Laser‐based and thermal studies of stress corrosion in vitreous silica , 1985 .
[58] Jack H. Campbell,et al. Effects of OH content, water vapor pressure, and temperature on sub-critical crack growth in phosphate glass , 2000 .
[59] Eamonn F. Healy,et al. Development and use of quantum mechanical molecular models. 76. AM1: a new general purpose quantum mechanical molecular model , 1985 .
[60] E. B. Shand. Experimental Study of Fracture of Glass:I, The Fracture Process , 1954 .
[61] Extended Charles–Hillig Theory for Stress Corrosion Cracking of Glass , 1992 .
[62] Samuel Glasstone,et al. The Theory Of Rate Processes , 1941 .
[63] C Gurney,et al. Delayed fracture in glass , 1947 .
[64] B. A. Proctor,et al. The strength of fused silica , 1967, Proceedings of the Royal Society of London. Series A. Mathematical and Physical Sciences.
[65] Subcritical crack growth in silica aerogel , 2004 .
[66] F. W. Preston. THE TIME FACTOR IN THE TESTING OF GLASSWARE , 1935 .
[67] B. Lawn. Diffusion-controlled subcritical crack growth in the presence of a dilute gas environment , 1974 .
[68] F Célarié,et al. Glass breaks like metal, but at the nanometer scale. , 2003, Physical review letters.
[69] S. Wiederhorn,et al. Do plastic zones form at crack tips in silicate glasses? , 2007 .
[70] A. Evans,et al. Analysis of the double cleavage drilled compression specimen for interface fracture energy measurements over a range of mode mixities , 1995 .
[71] F. Despetis,et al. Sub-critical crack growth in some phosphate glasses , 2008 .
[72] R. D. Southwick,et al. Strength and Static Fatigue of Abraded Glass Under Controlled Ambient Conditions: II, Effect of Various Abrasions and the Universal Fatigue Curve , 1959 .
[73] T. Zhu,et al. Stress-dependent molecular pathways of silica–water reaction , 2005 .
[74] Sheldon M. Wiederhorn,et al. Proof testing of ceramics , 1980 .
[75] W. Hillig. Model of effect of environmental attack on flaw growth kinetics of glass , 2007 .
[76] W. Wong-Ng,et al. Molecular orbital study of an environmentally enhanced crack growth process in silica , 1994 .
[77] M. J. Adams. Fracture of brittle solids (2nd edition): Brian Lawn , 1994 .